Material Notes:
BRC 409002 is a medium impact high flow injection molding compound designed for ease of process along with excellent weathering characteristics.Information Provided by Bayshore Vinyl Compounds Inc.
Physical Properties Metric English Comments
Specific Gravity 1.41 g/cc
1.41 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 80
80
ASTM D2240
Tensile Strength at Break 40.0 MPa
5800 psi
ASTM D638
Tensile Modulus 2.55 GPa
370 ksi
ASTM D638
Flexural Yield Strength 73.1 MPa
10600 psi
ASTM D790
Flexural Modulus 2.62 GPa
380 ksi
ASTM D790
Izod Impact, Unnotched 8.01 J/cm
15.0 ft-lb/in
ASTM D256
Impact 3.8
3.8
Gardner [in-lb/mil]; ASTM D5420
Thermal Properties Metric English Comments
Heat Distortion Temperature 65.0 °C
149 °F
ASTM D648
Descriptive Properties Value Comments
Equilibrium Torque (metergrams) 1000
187°C, 65g