Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 12.0 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 12.0 GPa
1740 ksi
ISO 527-2
PolyOne OnForce™ LFT NN-40LGF/000 HS Natural Polyamide 66 (Nylon 66)
PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. ..
Tensile Modulus 12.0 GPa
1740 ksi
ASTM D638
Premix Premi-Glas® 1200-22 Fiberglass Reinforced Thermoset SMC
Premi-Glas® 1200-22 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st..
Tensile Modulus 12.0 GPa
1740 ksi
ASTM D638
Premix Premi-Glas® 1200-25 Fiberglass Reinforced Thermoset SMC
Premi-Glas® 1200-25 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st..
Tensile Modulus 12.0 GPa
1740 ksi
ASTM D638
Premix Premi-Glas® 1240-15 Fiberglass Reinforced Thermoset Thick Molding Compound
Premi-Glas® 1240-15 is a fiberglass reinforced thermoset Thick Molding Compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st..
Tensile Modulus 12.0 GPa
1740 ksi
ASTM D638
Premix Premi-Glas® 3101-10 Fiberglass Reinforced Thermoset BMC
Premi-Glas® 3101-10 is a fiberglass reinforced thermoset bulk molding compound for electrical circuit breakers, switchgear and other applications where fire retardance is required.Key features and ..
Tensile Modulus 12.0 GPa
1740 ksi
ASTM D638
Premix Premi-Glas® 3101-15 Fiberglass Reinforced Thermoset BMC
Premi-Glas® 3101-15 is a fiberglass reinforced thermoset bulk molding compound for electrical circuit breakers, switchgear and other applications where fire retardance is required.Key features and ..
Tensile Modulus 12.0 GPa

@Thickness 4.00 mm,
Temperature 23.0 °C
1740 ksi

@Thickness 0.157 in,
Temperature 73.4 °F
ISO 527-2
PolyOne Bergamid™ A70 G35 H U BK SO Polyamide 66 (Nylon 66)
Information provided by PolyOne
Tensile Modulus 12.0 GPa

@Thickness 4.00 mm,
Temperature 23.0 °C
1740 ksi

@Thickness 0.157 in,
Temperature 73.4 °F
ISO 527-2/1
PolyOne Bergamid™ A70 G35 UF SO Polyamide 66 (Nylon 66)
Information provided by PolyOne
Tensile Modulus 12.0 GPa
1740 ksi
ASTM D638
Gharda Chemicals GATONE™ 5330FC Polyetheretherketone (PEEK)  (discontinued **)
Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric..
Tensile Modulus 12.0 GPa
1740 ksi
ASTM D638
Premix Premi-Glas® 2103-10 CRSX Polyester BMC
Premi-Glas® 2103-10 CR-SX is a 10% glass reinforced thermoset Sheet Molding Compound designed for electrical switchgear and industrial circuit breaker applications. Key features and benefits are:U..
Tensile Modulus 12.0 GPa

@Temperature 23.0 °C
1740 ksi

@Temperature 73.4 °F
ISO 527
Victrex® ST™ ST45GL30 Polyetherketoneetherketoneketone (PEKEKK), 30% Glass Fiber Reinforced
Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, c..
Tensile Modulus 12.0 GPa
1740 ksi
ISO 527
Premix Thermoplastics PRE-ELEC® 12-032  (discontinued **)
PRE-ELEC 12-032 is a conductive thermoplastic compound based on a polyacetal copolymer with 20% carbon fiber. PRE-ELEC 12-032 exhibits excellent mechanical properties and electrical conductivity. Te..
Tensile Modulus 12.0 GPa
1740 ksi
1mm/min; ISO 527-2/1A
Celanese VECTRA E130G LCP, 30% Glass Reinforced  (Unverified Data**)
30% glass fiber filled/low injection pressureInformation provided by Celanese
Tensile Modulus 12.0 GPa
1740 ksi
ASTM D638
Glastic Laminates/Shapes Polyester, Channels and Structural Shapes (GPO3)
Data provided by Glastic Corporation.NEMA GPO-3. Average data - may vary with the size and shape of the electrical insulating structural product.
Tensile Modulus 12.0 GPa
1740 ksi
ISO 527-2
Solvay Specialty Polymers Amodel® HFFR-4133 Polyphthalamide (PPA), 33% Glass Fiber
Amodel® HFFR-4133 is a 33% glass-reinforced, halogen-free, flame retardant polyphthalamide (PPA) resin which offers enhanced processing capabilities for electrical and electronic applications. Th..
Tensile Modulus 12.0 GPa
1740 ksi
ISO 527 Type 1A
Solvay TECHNYL® A 20 V35 PA66, 35% glass fiber, DRY
Description: Flame retardant polyamide 66, reinforced with 35% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America.Product Applications: This ph..
Tensile Modulus 12.0 GPa
1740 ksi
ISO 527
Vyncolit 2940 W Novolac Phenolic
Mineral and glass fiber filled phenolic molding compound with excellent mechanical and thermal properties. USES: Multi-V pulleys and solenoid covers.Information provided by Vyncolit, a Sumitomo Bake..
Tensile Modulus 12.0 GPa
1740 ksi
dry; ISO 527-1/-2
EMS-Grivory Grivory® BG-40 HM PA6-GF40
Product description: Grilon BG-40 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 40% glass fibers. Grilon BG-40 HM has the following important prop..
Tensile Modulus 12.0 GPa
1740 ksi
ISO 527-1/-2
DSM Stanyl® TE250F6 (DAM) Nylon 46 30% Glass Reinforced, Heat Stabilized, Flame Retardant (North America)
Information provided by DSM Engineering Plastics.
Tensile Modulus 12.0 GPa
1740 ksi
ISO 527-1/-2
DSM Stanyl® TE250F9 Nylon 46-45% Glass Reinforced (European and Asian Grade) (Cond)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Tensile Modulus 12.0 GPa
1740 ksi
ISO 527-1/-2
DSM Stanyl® TW250F6 Nylon 46-30% Glass Reinforced (European Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Tensile Modulus 12.0 GPa
1740 ksi
dry; ISO 527-1/-2
EMS-Grivory Grivory® LV-50H FWA black 9225 PA12-GF50
Product description: Grilamid LV-50H FWA black 9225 is a 50 % glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combine..
Tensile Modulus 12.0 GPa
1740 ksi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® LVX-50H nat PA12-GF50
Product description: Grilamid LVX-50H natural is a 50% glass fiber reinforced, heat stabilized polyamide 12. Special characteristics of this injection molding product are: Very high stiffness and st..
Tensile Modulus 12.0 GPa
1740 ksi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® XE 4105 nat PA610-GF50
Product description: Grilamid XE 4105 natural is a 50% glass fiber reinforced, heat stabilized polyamide 610 (PA610) injection molding grade. This product is to a large extent based on renewable raw..
Tensile Modulus 12.0 GPa
1740 ksi
1[mm/min]; ISO 527-1/2
Akro-Plastic Akroloy® PA GF 40 (2845) PA 6.6 & PA6I/6T Conditioned, 40% Glass Filled
One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param..
Tensile Modulus 12.0 GPa
1740 ksi
1[mm/min]; ISO 527-1/2
Akro-Plastic Akromid® T1 GF 30 (3466) PPA Conditioned, 30% Glass Filled
The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high..
Tensile Modulus 12.0 GPa
1740 ksi
50mm/min; ISO 527-2/1A
Celanese VECTRA A115 LCP, 15% Glass Reinforced
Provides easier flow than A130. Slightly tougher, but may warp slightly more than A130 in some parts. 15% glass reinforced.Information provided by Celanese
Tensile Modulus 12.0 GPa
1740 ksi
1[mm/min]; ISO 527-1/2
Akro-Plastic Akromid® T1 GF 30 9 (3498) PPA Conditioned, 30% Glass Filled
The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high..
Tensile Modulus 12.0 GPa
1740 ksi
1mm/min; ISO 527-2/1A
Celanese FORTRON 1130L4 PPS, 30% Glass Reinforced  (Unverified Data**)
Fortron 1130L4 is a 30% glass-reinforced PPS that has excellent heat and chemical resistance. It is inherently flame-retardant and exhibits high hardness and a good balance of strength and stiffness..
Tensile Modulus 12.0 GPa
1740 ksi
ISO 527-2
Solvay Specialty Polymers Amodel® HFFR-4133 Polyphthalamide (PPA)  (Unverified Data**)
Amodel HFFR-4133 is a 33% glass-reinforced, halogen- free, flame retardant polyphthalamide (PPA) resin which offers enhanced processing capabilities for electrical and electronic applications. This ..