Mechanical Properties Metric English Comments
Tensile Modulus 12.0 GPa
1740 ksi
ISO 527-2
PolyOne OnForce™ LFT NN-40LGF/000 HS Natural Polyamide 66 (Nylon 66)
PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. ..
Tensile Modulus 12.0 GPa
1740 ksi
STN EN ISO 527-2
Plastcom SLOVAMID® 6 GF 25 FRC 4 PA6 reinforced with glass fiber, flame retarded
PA 6 for injection molding, reinforced with 25 % glass fiber, flame retarded with halogen free flame retardant. Main features: flammability according to UL 94 3 at 1,6mm, glow wire at 960°C. Applic..
Tensile Modulus 12.0 GPa
1740 ksi
ASTM D638
Premix Premi-Glas® 1200-15 Fiberglass Reinforced Thermoset SMC
Premi-Glas® 1200-15 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st..
Tensile Modulus 12.0 GPa
1740 ksi
ASTM D638
Premix Premi-Glas® 1200-20 Fiberglass Reinforced Thermoset SMC
Premi-Glas® 1200-20 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st..
Tensile Modulus 12.0 GPa
1740 ksi
ASTM D638
Premix Premi-Glas® 1200H-15 Polyester SMC
Premi-Glas® 1200H-15 is a 15% fiberglass-reinforced, thermoset, Sheet Molding Compound designed for applications where good arc resistance and dielectric strength are required and UL 94 HB flame re..
Tensile Modulus 12.0 GPa
1740 ksi
ASTM D638
Premix Premi-Glas® 1200H-22 Fiberglass Reinforced Thermoset SMC
Premi-Glas® 1200H-22 is a fiberglass reinforced thermoset sheet molding compound for general purpose and HVAC applications requiring thermal stability and stiffness.Key features and benefits are:Go..
Tensile Modulus 12.0 GPa
1740 ksi
ASTM D638
Premix Premi-Glas® 1240-15 Fiberglass Reinforced Thermoset Thick Molding Compound
Premi-Glas® 1240-15 is a fiberglass reinforced thermoset Thick Molding Compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st..
Tensile Modulus 12.0 GPa
1740 ksi
ASTM D638
Premix Premi-Glas® 2204-30 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2204-30 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
Tensile Modulus 12.0 GPa
1740 ksi
ASTM D638
Premix Premi-Glas® 3200-30 Fiberglass Reinforced SMC
Description: Premi-Glas® 3200-30 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di..
Tensile Modulus 12.0 GPa

@Temperature 23.0 °C
1740 ksi

@Temperature 73.4 °F
ISO 527-2/1
PolyOne Bergamid™ B70 W25 G45 H Polyamide 6 (Nylon 6)
Information provided by PolyOne
Tensile Modulus 12.0 GPa
1740 ksi
ASTM D638
Glastic Laminates/Shapes UTR Glass-Mat-Reinforced, Mineral Filled Polyester Laminate
Data provided by Glastic Corporation.NEMA GPO-3/GPO-3P. Developed for transit industry where smoke generation and toxicity are of primary concern.
Tensile Modulus 12.0 GPa
1740 ksi
1 mm/min; ISO 527-1,-2
Lanxess Durethan® BKV 140 DUS008 000000 Nylon 6, 40% Glass Fiber
PA 6, 40% glass fibers, injection molding, impact modifiedInformation provided by LANXESS.
Tensile Modulus 12.0 GPa
1740 ksi
ISO 527-1, -2; 1 mm/min
Lanxess Pocan® T 7141 000000 PET + PBT, 40% Glass Fiber/Mineral
PET + PBT, 40% glass fibers/mineral, injection molding, improved flowability, high thermal dimensional stabilityInformation provided by LANXESS.
Tensile Modulus 12.0 GPa
1740 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Valox® ENH8560 PBT+PET (Europe-Africa-Middle East)
Non-Brominated & Non-Chlorinated Flame Retardant, 30% Glass fiber reinforced PBT/PET blend
Tensile Modulus 12.0 GPa
1740 ksi
ASTM D638
Lubrizol Isoplast® 101LGF40NAT Engineering Thermoplastic Polyurethane Resin
Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009.
Tensile Modulus 12.0 GPa
1740 ksi
ASTM D638
Lubrizol Isoplast® 2540 Engineering Thermoplastic Polyurethane Resin for Medical Applications
Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009.
Tensile Modulus 12.0 GPa
1740 ksi
ISO 527-1/-2
DSM Stanyl® 46HF5040 (COND) Nylon 46 40% Glass Reinforced, Heat Stabilized, Flame Retardant, High Flow (North America)
Information provided by DSM Engineering Plastics.
Tensile Modulus 12.0 GPa
1740 ksi
ISO 527-1/-2
DSM Stanyl® 46HF5040 Nylon 46-40% Glass Reinforced (European and Asian Grade) (Cond)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Tensile Modulus 12.0 GPa
1740 ksi
cond; ISO 527-1/-2
DSM Stanyl® TS250F8 PA46-GF40 FR
40% Glass Reinforced, Flame Retardant, Heat Stabilized
Tensile Modulus 12.0 GPa
1740 ksi
ISO 527-1/-2
DSM Stanyl® TS256F6 Nylon 46-30% Glass Reinforced (Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Tensile Modulus 12.0 GPa
1740 ksi
dry; ISO 527-1/-2
EMS-Grivory Grivory® LV-50H FWA black 9225 PA12-GF50
Product description: Grilamid LV-50H FWA black 9225 is a 50 % glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combine..
Tensile Modulus 12.0 GPa
1740 ksi
DAM; ISO 527-1/-2
DuPont Performance Polymers Zytel® HTN FG52G35HSLR BK011 Polyphthalamide (PPA)  (Unverified Data**)
Information provided by DuPont Performance Polymers
Tensile Modulus 12.0 GPa
1740 ksi
cond; ISO 527-1/-2
DSM EcoPaXX® Q-HG10 PA410-GF50
50% Glass Reinforced, Heat Stabilized
Tensile Modulus 12.0 GPa
1740 ksi
ISO 527
Eurotec® Tecopet® PT70 GR30 NL100 XD70 PET, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), long-term heat stabilized, natural
Information provided by Eurotec®
Tensile Modulus 12.0 GPa
1740 ksi
50mm/min; ISO 527-2/1A
Celanese VECTRA E130G LCP, 30% Glass Reinforced
30% glass fiber filled / low injection pressureInformation provided by Celanese
Tensile Modulus 12.0 GPa
1740 ksi
ISO 527-1
Celanese Coolpoly® D3606 Thermally Conductive Polyamide 4,6  (discontinued **)
CoolPoly D series of thermally conductive plastics transfers heat, a characteristic previously unavailable in injection molding grade polymers. CoolPoly is lightweight, netshape moldable and allows ..
Tensile Modulus 12.0 GPa
1740 ksi
ASTM-D790
Polyram Polytron A35N01 Nylon 66, Chemically Coupled 35% Long Fiber
A CHEMICALLY COUPLED 35% LONG FIBER GLASS REINFORCED NATURAL NYLON 6.6 HEAT STABILIZED FOR INJECTIONInformation provided by Polyram Ram On Ind.
Tensile Modulus 12.0 GPa
1740 ksi
50mm/min; ISO 527-2/1A
Celanese VECTRA MT1305 LCP, 15% Glass Reinforced
Provides easier flow than MT1310. Slightly tougher, but may warp slightly more than MT1310 in some parts. 15% glass reinforced.Information provided by Celanese
Tensile Modulus 12.0 GPa
1740 ksi
ISO 527-1/-2
Lanxess Pocan® DP T 7140 LDS 000000 PBT + PET, 44% Mineral + L227Glass Fiber  (discontinued **)
PET+PBT, 44% glass fibers/mineral, injection molding, LDS, high thermal dimension stability
Tensile Modulus 12.0 GPa

@Temperature 23.0 °C
1740 ksi

@Temperature 73.4 °F
ISO 527
Victrex® PEEK 150GL30 Black Polyetheretherketone, 30% Glass Fiber Reinforced