Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DSM Akulon® K224-TG9/A Nylon 6-45% Glass Reinforced (European Grade) (Cond)  (discontinued **)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 50% Glass Fiber Filled
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Akulon® K224-TG9/A Nylon 6-45% Glass Reinforced (European Grade) (Cond)  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier film, stock shapes, convoluted tubes, and monofilament. Akulon XP is a high-productivity, high-performance PA6 grade for film extrusion processes. Medium viscosity, unreinforced or reinforced Akulon grades are used for various injection molding and blow molding applications. Akulon® Ultraflow® is a high-productivity, high-performance PA6 family for molding processes.Key applications for Akulon: Automotive: Intake manifold, Engine, Powertrain, Airbag containers, Exterior trim, Interior trim, Electrical components and connectorsConsumer durables: Power tools, Lawn and garden tools, Small appliances, Sports and leisure equipment, Furniture, Industrial Goods, TransportationE&E: Low voltage switch gear/power distribution, Lighting, Power connectorsFilm: Specialty and barrier filmsInformation provided by DSM.
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
(DAM); ISO 1183
Water Absorption 5.0 %
5.0 %
DAM; Sim. to ISO 62
Moisture Absorption at Equilibrium 1.5 %
1.5 %
Humidity Absorption (DAM); Sim. to ISO 62
Mechanical Properties Metric English Comments
Tensile Strength at Break 150 MPa
21800 psi
ISO 527-1/-2
Elongation at Break 4.0 %
4.0 %
ISO 527-1/-2
Tensile Modulus 9.50 GPa
1380 ksi
ISO 527-1/-2
Charpy Impact Unnotched 7.50 J/cm²

@Temperature -30.0 °C
35.7 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
11.5 J/cm²

@Temperature 23.0 °C
54.7 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 1.30 J/cm²

@Temperature -30.0 °C
6.19 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
3.50 J/cm²

@Temperature 23.0 °C
16.7 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
10°C/min (DAM); ISO 11357-1/-3
UL RTI, Electrical 65.0 °C

@Thickness 1.50 mm
149 °F

@Thickness 0.0591 in
UL746B
65.0 °C

@Thickness 0.750 mm
149 °F

@Thickness 0.0295 in
UL746B
UL RTI, Mechanical with Impact 65.0 °C

@Thickness 0.750 mm
149 °F

@Thickness 0.0295 in
UL746B
65.0 °C

@Thickness 1.50 mm
149 °F

@Thickness 0.0591 in
UL746B
UL RTI, Mechanical without Impact 65.0 °C

@Thickness 1.50 mm
149 °F

@Thickness 0.0591 in
UL746B
65.0 °C

@Thickness 0.750 mm
149 °F

@Thickness 0.0295 in
UL746B
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
IEC 60093
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
IEC 60093
Dielectric Constant 4.5

@Frequency 1e+6 Hz
4.5

@Frequency 1e+6 Hz
IEC 60250
14

@Frequency 100 Hz
14

@Frequency 100 Hz
IEC 60250
Dielectric Strength 20.0 kV/mm
508 kV/in
IEC 60243-1
Dissipation Factor 0.12

@Frequency 1e+6 Hz
0.12

@Frequency 1e+6 Hz
IEC 60250
0.30

@Frequency 100 Hz
0.30

@Frequency 100 Hz
IEC 60250
Comparative Tracking Index 600 V
600 V
IEC 60112
Descriptive Properties Value Comments
Injection molding Yes
Release Agent Yes
With Fillers Yes
Users viewing this material also viewed the following: