Covestro Desmopan® DP 3660DU Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Covestro
Trade Name Desmopan®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Desmopan® DP 3660DU Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Extrusion- and injection molding gradetransparent up to 6 mm wall thicknesshydrolysis-stabilisedwith special UV stabilizerswith release agentgood wear resistanceApplicationSports shoe solesHosesnon-reinforcedProfilesPreprocessingMax. Water content
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
Melt
1.23 g/cc
0.0444 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 98
98
3s; ISO 868
Hardness, Shore D 62
62
15s; ISO 868
Abrasion 23
23
mm³; ISO 4649
Compression Set 24 %

@Temperature 23.0 °C
24 %

@Temperature 73.4 °F
ISO 815
47 %

@Temperature 70.0 °C
47 %

@Temperature 158 °F
ISO 815
Thermal Properties Metric English Comments
Specific Heat Capacity 1.70 J/g-°C
0.406 BTU/lb-°F
Melt
Thermal Conductivity 0.139 W/m-K
0.965 BTU-in/hr-ft²-°F
Melt
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Processing Properties Metric English Comments
Melt Temperature 215 - 235 °C
419 - 455 °F
Mold Temperature 20.0 - 40.0 °C
68.0 - 104 °F
Ejection Temperature 50.0 °C
122 °F
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
India
Near East/Africa
South and Central America
Eff. thermal diffusivity (m²/s) 8.02E-08