Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Toyobo A3080A Thermoplastic Polyurethane Elastomer, Injection Grade

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Ether Grade
Manufacturer Toyobo
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Toyobo A3080A Thermoplastic Polyurethane Elastomer, Injection Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polyether type, featuring excellent resistance to hot water and fungus. Various grades of Toyobo polyurethane TPEs are used in auto parts, hoses, tubes, sporting goods, shoe soles, etc.Information provided by Toyobo Co., Ltd
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 82
82
ASTM D2240
Tensile Strength, Ultimate 39.0 MPa
5660 psi
ASTM D638
Tensile Strength, Yield 5.40 MPa

@Strain 100 %
783 psi

@Strain 100 %
ASTM D638
Elongation at Break 510 %
510 %
ASTM D638
Tear Strength 88.0 kN/m
502 pli
ASTM D624
Taber Abrasion, mg/1000 Cycles 10
10
H22
Compression Set 35 %
35 %
ASTM D395B
Thermal Properties Metric English Comments
Vicat Softening Point 90.0 °C
194 °F
ASTM D1525
Brittleness Temperature <= -65.0 °C
<= -85.0 °F
ASTM D746