Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Apec® 2000 Polycarbonate
(discontinued **) Key Features:UnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionCoatingBlow moldingCalanderingTransfer moldingThermoformingInformation provided by Bay.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | ASTM C351 |
LyondellBasell Moplen HP400H Polypropylene Homopolymer Description: Moplen HP400H is a homopolymer for extrusion applications. Moplen HP400H exhibits easy processability and a good stiffness/impact balance at ambient temperature. The main applications .. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | |
Zell-Metall Engineering Plastics Zellamid 1200 G Zellamid® 1200 G is manufactured by an activated anionic reaction. Finished and semi-finished parts are produced by a static cast process. This process makes it possible to produce a material wit.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | |
Zell-Metall Engineering Plastics Zellamid 1200 G at 50% RH Zellamid® 1200 G is manufactured by an activated anionic reaction. Finished and semi-finished parts are produced by a static cast process. This process makes it possible to produce a material wit.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | DIN 52612 |
Zell-Metall Engineering Plastics Zellamid 202 (PA 6) Zellamid® 202 is a tough material with high resistance to abrasion and impact. It features good mechanical properties. By water absorption the excellent shock and vibration resistance is increased... |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Apec® 1695 Polycarbonate Easy flowingeasy to demoldsoftening temperature (VST/B 120)=158 °CPreprocessingMax. Water content |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Apec® 1895 Polycarbonate Easy flowingeasy to demoldsoftening temperature (VST/B 120)=183 °CPreprocessingMax. Water content |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Desmopan® 481 Polyurethane injection molding gradefree from plasticizersgrease and oil-resistantlow compression sethigh elasticitygood heat resistanceEasy releaseApplicationRoller coatingSealsmembranesAutomotive engineeringPr.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Desmopan® DP 2586A Polyurethane Extrusion- and injection molding gradedoes not contain any anti-hydrolysis agentfood contact applications are possiblecontact our HSEQ departmentBeadsApplicationBlown filmsPreprocessingMax. Water co.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Desmopan® DP 2786A Polyurethane Coating gradedoes not contain any anti-hydrolysis agentfood contact applications are possiblecontact our HSEQ departmentApplicationTextile coatingPreprocessingMax. Water content |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Desmopan® DP 9662DU Polyurethane Extrusion- and injection molding gradewith special UV stabilizerstransparent up to 6 mm wall thicknessvery good hydrolysis and microbial resistanceApplicationSki boot shellsHosesnon-reinforcedPrepro.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Desmopan® DP 9665DU Polyurethane Extrusion- and injection molding gradewith special UV stabilizerstransparent up to 6 mm wall thicknessvery good hydrolysis and microbial resistanceApplicationSki boot shellsHosesnon-reinforcedPneuma.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Desmopan® W DP 85085A Polyurethane injection molding gradeno yellowing under the action of UV lightimproved microbial resistancegood low-temperature flexibilityImproved hydrolysis resistanceApplicationautomotive interior applications.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Makroblend® KU 2-7608 Polycarbonate + PBT, Mineral Filled Impact Grade ISO 7792-1-PC/PBT,MHPR,-030,MD10(PC+PBT)-blendsimpact modifiedInjection molding grade 10% mineral filledPreprocessingMax. Water content |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Makrolon® 2806 Polycarbonate ISO 7391-PC,M,(,,)-09-9MVR (300 °C/1.2 kg) 9.5 cm3/10 minFood contact qualityMedium viscosityGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CAvailable in transparenttran.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Makrolon® 2856 Polycarbonate ISO 7391-PC,MR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 9.5 cm3/10 minFood contact qualityMedium viscosityEasy releaseGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CAva.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Makrolon® 3106 Polycarbonate ISO 7391-PC,M,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minFood contact qualityHigh viscosityGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CExtrusionAvailable.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Makrolon® 3107 Polycarbonate ISO 7391-PC,MLR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minGeneral purposeHigh viscosityUV stabilizedEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in transpare.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Makrolon® 3156 Polycarbonate ISO 7391-PC,MR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minFood contact qualityHigh viscosityEasy releaseGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CExtru.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Makrolon® 6265 Polycarbonate, Flame Retardant Grade ISO 7391-PC,MFR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 19 cm3/10 minFlame retardantUL 94V-0/1.5 mmLow viscosityEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in opaque co.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Makrolon® 6457 Polycarbonate, Flame Retardant Grade MVR (300 °C/1.2 kg) 12.5 cm3/10 minUL 94V-0/3.0 mmUV stabilizedeasy releaseinjection moldingavailable in transparent, translucent and opaque colorsPreprocessingMax. Water content |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Makrolon® 6585 Polycarbonate, Flame Retardant Grade ISO 7391-PC,MFR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minFlame retardantUL 94V-0/1.2 mm5VA/3.0 mm and 5VB (WT) /2.0 mmHigh viscosityEasy releaseInjection molding - Melt temperature 28.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Makrolon® Rx1805 Polycarbonate ISO 7391-PC,M,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minMedical devicesLipid resistantsuitable for sterilization with high-energy radiationComplies with the requirements of FDA-modifie.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Makrolon® WB1239 Polycarbonate ISO 7391-PC,B,(,,)-05-9Global gradeMVR (300 °C/1.2 kg) 2.5 cm3/10 minBlow moldingHigh viscosityBranchedFood contact qualityExtrusion blow moldingInjection stretch blow moldingAvailable in transpare.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Makrolon® 1248 Polycarbonate, Impact Grade ISO 7391-PC,MP,(,,)-09-9Formerly Makrolon KU1-1248MVR (300 °C/1.2 kg) 7.0 cm3/10 minFood contact qualityMedium viscosityImpact modifiedInjection molding - Melt temperature 280 - 320 °CAvailable in.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Makrolon® 2456 Polycarbonate ISO 7391-PC,MR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 19 cm3/10 minFood contact qualityLow viscosityEasy releaseGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CAvailab.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | |
BASF Ultramid® A3K BK 00464 PA66 (Conditioned) Description: Easy flowing injection-molding grade for fast processing. Uses include highly stressed technical parts such as bearings and gear wheels; also electrically insulating parts such as termi.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Makrolon® Rx1452 Polycarbonate ISO 7391-PC,M,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minMedical devicesLipid resistantsuitable for sterilization with high-energy radiationComplies with the requirements of FDA-modifie.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | |
BASF Ultramid® B3S BK00464 PA6 (Dry) Ultramid B3S BK00464 is an easy flowing, pigmented black, finely crystalline injection molding PA6 grade. It conforms to FDA requirements of 21 CFR 177.1500. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Mfr. internal test |
Ascend Performance Materials VYDYNE® 21SP Nylon, General Purpose 1.4% Deformation under 14 MPa (2000 psi) load.Typical property data. VYDYNE is a registered trademark of Solutia Inc. |