Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Apec® 1700 Polycarbonate
(discontinued **) Key Features:UnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionCoatingBlow moldingCalanderingTransfer moldingThermoformingInformation provided by Bay.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Apec® 2000 Polycarbonate
(discontinued **) Key Features:UnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionCoatingBlow moldingCalanderingTransfer moldingThermoformingInformation provided by Bay.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | |
Zell-Metall Engineering Plastics Zellamid 1200 G Zellamid® 1200 G is manufactured by an activated anionic reaction. Finished and semi-finished parts are produced by a static cast process. This process makes it possible to produce a material wit.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | |
Zell-Metall Engineering Plastics Zellamid 1200 G at 50% RH Zellamid® 1200 G is manufactured by an activated anionic reaction. Finished and semi-finished parts are produced by a static cast process. This process makes it possible to produce a material wit.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | DIN 52612 |
Zell-Metall Engineering Plastics Zellamid 202 (PA 6) Zellamid® 202 is a tough material with high resistance to abrasion and impact. It features good mechanical properties. By water absorption the excellent shock and vibration resistance is increased... |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Apec® 1795 Polycarbonate Easy flowingeasy to demoldsoftening temperature (VST/B 120)=173°CPreprocessingMax. Water content |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Apec® 1800 Polycarbonate Basic gradesoftening temperature (VST/B 120)=185 °CPreprocessingMax. Water content |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Apec® 2095 Polycarbonate Easy flowingeasy to demoldsoftening temperature (VST/B 120)=203 °CPreprocessingMax. Water content |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Desmopan® DP 1080A Polyurethane injection molding gradefree from plasticizershard - soft systemsTechnical partsAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covest.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Desmopan® DP 1485A Polyurethane Extrusion- and injection molding gradesuitable for extrusion blow moldingvery large processing windowhigh melt stabilityBeadsApplicationBellowsHosesnon-reinforcedProfilesInjection molded engineering.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Desmopan® DP 3695AU Polyurethane Extrusion- and injection molding gradetransparent up to 6 mm wall thicknesshydrolysis-stabilisedwith special UV stabilizerswith release agentgood wear resistanceApplicationSports shoe solesHosesnon-.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Desmopan® DP 5080A Polyurethane injection molding gradeimproved microbial resistanceImproved hydrolysis resistanceApplicationSealsmembraneshard - soft systemsPreprocessingMax. Water content |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Desmopan® DP 8798A Polyurethane injection molding gradewith special UV stabilizersEasy releaseshort cycle timesApplicationSports shoe solesPreprocessingMax. Water content |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Desmopan® DP 9370A Polyurethane Extrusion- and injection molding gradevery good hydrolysis and microbial resistancegood low-temperature flexibilityfree from plasticizershigh moisture vapor transmission rateApplicationbreathable fi.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Desmopan® DP 9395AU Polyurethane Extrusion- and injection molding gradewith special UV stabilizersvery good hydrolysis and microbial resistancegood low-temperature flexibilityApplicationPneumatic hosesProfilesCable sheathingsInject.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Makrolon® 1899* Polycarbonate, Impact Grade Formerly Makrolon DP1-1899MVR (300 °C/1.2 kg) 15.5 cm³/10 minspecial flame retardant systemUL 94V-0/0.75 mmImpact modifiedMedium viscosityEasy releaseVicat softening temperature 50 N; 50 °C/h = 1.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Makrolon® 2665 Polycarbonate, Flame Retardant Grade ISO 7391-PC,MFR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12.5 cm3/10 minChlorine- and bromine-free flame retardantUL 94V-2/1.5 mm and 3.0 mmMedium viscosityEasy releaseInjection molding - Melt temp.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Makrolon® 3103 MAS157 Polycarbonate ISO 7391-PC,EL,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minExtrusionHigh viscosityUV stabilizedAvailable in color code 550115 onlySolid sheetCorrugated sheetPreprocessingMax. Water conte.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Makrolon® 3106 Polycarbonate ISO 7391-PC,M,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minFood contact qualityHigh viscosityGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CExtrusionAvailable.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Makrolon® 6265 Polycarbonate, Flame Retardant Grade ISO 7391-PC,MFR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 19 cm3/10 minFlame retardantUL 94V-0/1.5 mmLow viscosityEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in opaque co.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Makrolon® 6455 Polycarbonate, Flame Retardant Grade MVR (300 °C/1.2 kg) 12.5 cm3/10 minUL 94V-0/3.0 mmeasy releaseinjection moldingavailable in transparenttranslucent and opaque colorsPreprocessingMax. Water content |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Makrolon® LQ3147 Polycarbonate ISO 7391-PC,MLR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minOptical lensHigh viscosityUV stabilizedEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in clear tints .. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Makrolon® WB1239 Polycarbonate ISO 7391-PC,B,(,,)-05-9Global gradeMVR (300 °C/1.2 kg) 2.5 cm3/10 minBlow moldingHigh viscosityBranchedFood contact qualityExtrusion blow moldingInjection stretch blow moldingAvailable in transpare.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | |
Hippe PA 66 Nylon 66 The polyamide with high degree of hardness, stiffness, scuff strength and stability of shape under heat. Preferred polyamide for components subjected to high load and heat stress in electrical, mec.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Makrolon® 1243 Polycarbonate ISO 7391-PC,ELS,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minExtrusionHigh viscosityBranchedUV stabilizedEasy releaseAvailable in color code 550111onlyMulti wall sheet/profilesPreprocessi.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Makrolon® OD2015 Polycarbonate Global gradeOptical storage mediaLow viscosityEasy releaseHigh purityInjection moldingAvailable in natural color onlyPreprocessingMax. Water content |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | |
BASF Ultramid® B3K PA6 (Conditioned) Ultramid B 3K is an easy flowing, stabilized for fast processing, grade of nylon 6. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | |
BASF Ultramid® C3U BK 23079 PA6/66 FR (Conditioned) Description: Injection-molding grade with improved flame retardance (free from halogens and phosphorus), used e.g. for impact resistant electrically insulating parts such as contact bases and plug c.. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | |
BASF Ultramid® C3U PA66/6 (Conditioned) Ultramid C3U is an injection molding, general purpose PA66/6 grade with improved flame retardance. |
|||
Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
Covestro Makrolon® KU1-1230* Polycarbonate ISO 7391-PC,EFL,(,,)-09-9Developmental productMVR (300 °C/1.2 kg) 8.5 cm3/10 minFlame retardant16 mm Triple wall sheet/B1 classification (DIN 4102)Medium viscosityUV stabilizedExtrusionAs of 1 Sept.. |