Clariant Renol ABS5475 ABS, General Purpose, Low Gloss

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer Clariant
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Clariant Renol ABS5475 ABS, General Purpose, Low Gloss.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Clariant Masterbatches
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0060 cm/cm
0.0060 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 39.3 MPa
5700 psi
ASTM D638
Elongation at Break 40 %
40 %
ASTM D638
Flexural Modulus 2.07 GPa
300 ksi
ASTM D790
Izod Impact, Notched 1.60 J/cm

@Temperature 22.8 °C
3.00 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 94.4 °C
202 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 87.8 °C
190 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 216 - 249 °C
420 - 480 °F
Mold Temperature 65.6 - 93.3 °C
150 - 200 °F
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
8.27 - 13.8 MPa
1200 - 2000 psi
Initial
Back Pressure 0.345 - 1.72 MPa
50.0 - 250 psi
Shot Size 30 - 80 %
30 - 80 %
Screw Speed 20 - 100 rpm
20 - 100 rpm