Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 94.4 °C | 202 °F | Unannealed; ASTM Data |
Americas Styrenics Styron® 613 Polystyrene
(discontinued **) STYRON® 613 high heat, high strength general purpose polystyrene is typically used in applications requiring a clear, tough part such as office products and magnetic media enclosures. It offers goo.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 94.4 °C | 202 °F | Unannealed; ASTM Data |
Americas Styrenics Styron® 663 Polystyrene
(discontinued **) STYRON® 663 general purpose polystyrene resin is an additive free resin with excellent strength, clarity, and high heat resistance. When used unmodified for the manufacture of food contact articles.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 94.4 - 113 °C | 202 - 235 °F | Average value: 102 °C Grade Count:8 |
Overview of materials for Acrylic, Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Heat Resistant, Molded". Each property range of values reported is minimum and maximum values o.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 94.4 °C | 202 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® ABS LE WT Availability: North AmericaForms: PelletsFeatures: Low Extractables and Medium Impact ResistanceAppearance: WhiteInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 94.4 °C | 202 °F | ASTM D648 |
ExxonMobil PP7505KNE2 Polypropylene Homopolymer Product Description: A medium to high impact copolymer designed for injection molded large consumer and industrial parts requiring high melt flow rate.Availability: North America Features:Balanced .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 94.4 °C | 202 °F | ASTM D648 |
ExxonMobil PP7855E1 Polypropylene Homopolymer Product Description: A high crystallinity, medium impact strength copolymer resin with high melt flow rate and good processing attributes. It is designed for injection-molded automotive interior ap.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 94.4 °C | 202 °F | ASTM D648 |
Clariant Renol ABS5475 ABS, General Purpose, Low Gloss Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 94.4 °C | 202 °F | ASTM D648 |
Americas Styrenics STYRON® 668 High Heat Crystal Polystyrene Product CharacteristicsHigh heatGood balance of flow and toughnessFood Contact CompliantUL Classification 94HBTypical ApplicationsDisposable cutleryCD and DVD jewel boxesInformation provided by Amer.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 94.4 °C | 202 °F | ASTM D648 |
Gromax Evasin EV-3201V Ethylene-Vinyl Alcohol Copolymer Unmodified random Co-Polymer of [Ethylene-Vinyl alcohol], designed for therm-plastic processing into Sheets and Foils with high Oxygen and Aroma Barrier EffectInformation provided by Gromax Enterpri.. |