Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chesterton ARC S1HB Sprayable high-viscosity, 100% solids, advanced coating

Category Polymer , Thermoset , Epoxy
Manufacturer Chesterton
Trade Name ARC
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chesterton ARC S1HB Sprayable high-viscosity, 100% solids, advanced coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
An advanced composite formulated to protect concrete and metal surfaces from corrosion and chemical attack. It is normally applied at a thickness of 1-2 mm (40-80 mils) per coat. However, greater single coat film thickness is achievable when spray applied. Non-shrinking, 100% solids. ARC S1HB is a high viscosity, high performance composite lining that is designed to be a spray applied but may also be applied by brush. ARC S1HB allows for uniform coverage over rough surfaces and yields excellent immersion exposures. The cured ARC S1HB provides a barrier film with adhesion and resistance to corrosion.Benefits:High build capability for coverage over irregular surfaces.Outlasts conventional paints and coatingsLong pot life allow for ease of use100% solids, no shrinkage on cureOutstanding adhesion insures reliable performanceAble to be high voltage spark tested for pinhole free films. Suggested Uses:Bar Screen ChambersJunction/Splitter Boxescollection system PipingDigestersSewer PipingWaste water ClarifiersManholesThickener Tanks”Other” Concrete and Metal StructuresInformation provided by Chesterton
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
Cured
Mechanical Properties Metric English Comments
Hardness, Shore D 85
85
ASTM D2240
Tensile Strength at Break 38.7 MPa
5610 psi
ASTM D638
Elongation at Break 6.0 %
6.0 %
ASTM D638
Flexural Strength 57.6 MPa
8360 psi
ASTM D790
Flexural Modulus 2.96 GPa
430 ksi
ASTM D790
Compressive Strength 85.43 MPa
12390 psi
ASTM D695
Adhesive Bond Strength 10.1 MPa
1460 psi
Dry Concrete; ASTM D4541
>= 13.8 MPa
>= 2000 psi
Metal; ASTM D4541
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 52.0 °C
126 °F
Wet Service
80.0 °C
176 °F
Dry Service
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 43.0 °C
2.00 hour

@Temperature 109 °F
Tack Free
360 min

@Temperature 32.0 °C
6.00 hour

@Temperature 89.6 °F
Tack Free
420 min

@Temperature 25.0 °C
7.00 hour

@Temperature 77.0 °F
Tack Free
480 min

@Temperature 43.0 °C
8.00 hour

@Temperature 109 °F
Light Load
600 min

@Temperature 10.0 °C
10.0 hour

@Temperature 50.0 °F
Tack Free
960 min

@Temperature 43.0 °C
16.0 hour

@Temperature 109 °F
Overcoat End
1080 min

@Temperature 32.0 °C
18.0 hour

@Temperature 89.6 °F
Light Load
1440 min

@Temperature 43.0 °C
24.0 hour

@Temperature 109 °F
Full Load
1800 min

@Temperature 32.0 °C
30.0 hour

@Temperature 89.6 °F
Overcoat End
1920 min

@Temperature 25.0 °C
32.0 hour

@Temperature 77.0 °F
Light Load
2160 min

@Temperature 25.0 °C
36.0 hour

@Temperature 77.0 °F
Overcoat End
2160 min

@Temperature 32.0 °C
36.0 hour

@Temperature 89.6 °F
Full Load
2400 min

@Temperature 10.0 °C
40.0 hour

@Temperature 50.0 °F
Light Load
2880 min

@Temperature 43.0 °C
48.0 hour

@Temperature 109 °F
Full Chemical
3360 min

@Temperature 10.0 °C
56.0 hour

@Temperature 50.0 °F
Overcoat End
3600 min

@Temperature 25.0 °C
60.0 hour

@Temperature 77.0 °F
Full Load
4320 min

@Temperature 10.0 °C
72.0 hour

@Temperature 50.0 °F
Full Load
4320 min

@Temperature 32.0 °C
72.0 hour

@Temperature 89.6 °F
Full Chemical
5400 min

@Temperature 25.0 °C
90.0 hour

@Temperature 77.0 °F
Full Chemical
7200 min

@Temperature 10.0 °C
120 hour

@Temperature 50.0 °F
Full Chemical
Descriptive Properties Value Comments
Color Light Gray