BCC Products BC 32 Fibrous Glass

Category Ceramic , Glass , Glass Fiber , Other Engineering Material , Composite Fibers
Manufacturer BCC Products
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BCC Products BC 32 Fibrous Glass.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BC 32, microglass milled fibers will increase the mechanical strengths, such as impact strength, tensile strength, compressive strength, and flexural strength in plastic tooling compounds. They are used as a reinforcement to both improve dimensional stability as well as increase heat distortion at elevated temperatures.Information provided by BCC Products, Inc.
Physical Properties Metric English Comments
Particle Size 8.0 - 25 µm
8.0 - 25 µm
fiber diameter
Descriptive Properties Value Comments
Appearance off white powder
Contamination Free of foreign matter, including nodulated and unmilled fibers
Fiber Length 75 µm mean, <10 µm 1%, >320 µm 1%
Sizing cationic sized 1/32