CMT Materials HYTAC® XTL Tough Thermoplastic Syntactic Foam

Category Polymer , Thermoplastic
Manufacturer CMT Materials
Trade Name HYTAC®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CMT Materials HYTAC® XTL Tough Thermoplastic Syntactic Foam.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HYTAC®-XTL was developed to offer an improved surface quality after machining when compared to our popular HYTAC-B1X. This is particularly important when working with sticky or transparent plastics due to the challenge of polishing any thermoplastic syntactic material. Thermoplastic syntactic foams from CMT have become a good choice for plug assist due to their low thermal conductivity and ability to withstand chips and dings associated with any typical thermoforming process.In addition to enhanced surface quality, HYTAC-XTL has these outstanding attributes: The highest toughness ratings for any syntactic foamGood machinability with no dustExcellent where edge definition and detail are required Low thermal conductivityLow coefficient of thermal expansionExcellent material distribution Variety of Shapes and Sizes: The material is provided in standard sized rods or sheets, but may be custom molded to meet specific needs. Applications: HYTAC-XTL is the first material to combine the machined surface quality of an epoxy syntactic with the durability and dust free machining of a thermoplastic syntactic foam. Excellent surface characteristics optimize material distribution with most plastics. Recommended for use with PP, PET, PE, APET, CPET, HIPS, OPS, PETG, PLA, PS, PVC and RPET Information Provided by CMT Materials, Inc.
Physical Properties Metric English Comments
Density 0.721 g/cc
0.0260 lb/in³
Mechanical Properties Metric English Comments
Flexural Toughness 0.159 MPa
23.0 psi
ASTM D790
Compressive Strength 70.43 MPa
10220 psi
Thermal Properties Metric English Comments
CTE, linear 57.6 µm/m-°C
32.0 µin/in-°F
Thermal Conductivity 0.170 W/m-K
1.18 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 177 °C
350 °F
Descriptive Properties Value Comments
Color Mauve