Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Toughness | 0.159 MPa | 23.0 psi | ASTM D790 |
CMT Materials HYTAC® XTL Tough Thermoplastic Syntactic Foam HYTAC®-XTL was developed to offer an improved surface quality after machining when compared to our popular HYTAC-B1X. This is particularly important when working with sticky or transparent plastic.. |