A. Schulman POLYFLAM™ RCP 500 C

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYFLAM™ RCP 500 C.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolyflam® RCP 500C is an economical flame-retardant concentrate based in low-density polyethylene that features excellent dispersion and processing stability up to 550°F. ApplicationRCP 500C is recommended for use in low, linear and high-density polyethylene. It can be used with equal success in extrusion, blow molding, structural foam and film applications. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.60 g/cc
1.60 g/cc
ASTM D792
Melt Flow 4.0 - 8.0 g/10 min
4.0 - 8.0 g/10 min
ASTM D1238