Mechanical Properties Metric English Comments
Compressive Strength 70.43 MPa
10220 psi
CMT Materials HYTAC® XTL Tough Thermoplastic Syntactic Foam
HYTAC®-XTL was developed to offer an improved surface quality after machining when compared to our popular HYTAC-B1X. This is particularly important when working with sticky or transparent plastic..