Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ascend Performance Materials Vydyne® 47 Nylon 66, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Ascend Performance Materials (formerly Solutia)
Trade Name VYDYNE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ascend Performance Materials Vydyne® 47 Nylon 66, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Vydyne® 47 Nylon resins are general purpose polyamide, impact modified grades. They are available in natural, black and heat stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 47H was formulated to provide thermal endurance when used in applications in which continuous or extended high temperature exposure is anticipated.Information provided by Ascend
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ISO 1183
Water Absorption 1.2 %
1.2 %
24 hrs; ISO 62
Linear Mold Shrinkage 0.018 cm/cm

@Thickness 2.00 mm
0.018 in/in

@Thickness 0.0787 in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.016 cm/cm

@Thickness 2.00 mm
0.016 in/in

@Thickness 0.0787 in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 40.0 MPa
5800 psi
ISO 527
Tensile Strength, Yield 45.0 MPa
6530 psi
ISO 527
Elongation at Break 60 %
60 %
ISO 527
Flexural Strength 24.0 MPa
3480 psi
ISO 178
Flexural Modulus 0.783 GPa
114 ksi
ISO 178