Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.721 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.721 g/cc
0.0260 lb/in³
Zircar Zirconia M-45 Alumina Boards, Discs & Cylinders Insulation
Zircar alumina insulation Type M Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with with silica binders in BusterM that form a thermal shock resistant mullite..
Density 0.721 g/cc
0.0260 lb/in³
Dry
Unifrax Fiberfrax® LDS AL-Moldable Moldable Insulation
Fiberfrax LDS and LDS-AL moldables consist of Fiberfrax ceramic fibers dispersed in a sticky water-based refractory binder. These materials have a putty-like consistency which permits application b..
Density 0.721 g/cc
0.0260 lb/in³
Zircar Zirconia M-45 Alumina Boards, Discs & Cylinders Insulation
Zircar alumina insulation Type M Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with with silica binders in BusterM that form a thermal shock resistant mullite..
Density 0.721 g/cc
0.0260 lb/in³
CMT Materials HYTAC® XTL Tough Thermoplastic Syntactic Foam
HYTAC®-XTL was developed to offer an improved surface quality after machining when compared to our popular HYTAC-B1X. This is particularly important when working with sticky or transparent plastic..
Density 0.721 g/cc
0.0260 lb/in³
ASTM C134
BNZ Materials BNZ-25 Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Density 0.721 g/cc
0.0260 lb/in³
ASTM D1056
ACC Magnifoam™ MFSILTEC™-HD MTI Silicones Silicone Foam
Part of the Amber Chemical Group. Data provided by manufacturer.
Density >= 0.721 g/cc
>= 0.0260 lb/in³
Monmouth Rubber & Plastics Superbounce 90 NEO/SBR
Information provided by Monmouth Rubber & Plastics Corp.
Density 0.721 g/cc
0.0260 lb/in³
Pyrotek Wollite 45 Insulating Castable
Wollite material is a solid, light weight mineral foam which is stable during its preparation and during subsequent curing and drying. Because of the foam properties it is well suited for casting c..
Density 0.721 g/cc
0.0260 lb/in³
BNZ Materials 2645LI Insulating Aggregate
BNZ manufactures a variety of insulating and dense castable refractories to meet the exacting needs of the high temperature processing industries. These hydraulic setting products are suitable for i..
Copyright © lookpolymers.com All Rights Reserved