Material Notes:
Recovered polypropylene and polyethylene compositeInformation provided by Breplast S.p.A.
Physical Properties Metric English Comments
Density >= 0.930 g/cc
>= 0.0336 lb/in³
ISO 1183-1
Melt Flow 1.5 - 3.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.5 - 3.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
4.0 - 6.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
4.0 - 6.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 5.00 MPa
725 psi
ISO 527
Tensile Strength, Yield 5.00 MPa
725 psi
ISO 527
Elongation at Break 15 %
15 %
ISO 527
Flexural Strength 23.0 MPa
3340 psi
ISO 178
Flexural Modulus 0.890 GPa
129 ksi
ISO 178
Izod Impact, Notched 0.0900 J/cm
0.169 ft-lb/in
ISO 180
Thermal Properties Metric English Comments
Vicat Softening Point 126 °C
259 °F
A50; ISO 306
Descriptive Properties Value Comments
Color Dark Grey