Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 4.0 g/10 min @Load 3.80 kg, Temperature 230 °C |
4.0 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycolac® FR15 ABS Flame retardant ABS (non-PBBE additive). Good property/toughness. Excellent moldability. UL94 V-0/5VA rated. |
|||
Melt Flow | 4.0 g/10 min @Load 3.80 kg, Temperature 230 °C |
4.0 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycolac® FR15 ABS (Asia Pacific) Flame retardant ABS (non-PBBE additive). Good property/toughness. Excellent moldability. UL94 V-0/5VA rated. |
|||
Melt Flow | 4.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Network Polymers SAN 280 Water Clear Description: SAN - Styrene Acrylonitrile Transparent Engineering ThermoplasticInformation provided by Network Polymers Inc. |
|||
Melt Flow | 4.0 g/10 min @Load 5.00 kg, Temperature 230 °C |
4.0 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
Premix Thermoplastics PRE-ELEC® PP 1386 PRE-ELEC PP 1386 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
Melt Flow | 4.0 - 6.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.0 - 6.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 4020R (20405) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 4.0 - 6.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.0 - 6.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 4435S (35405) Medium Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 4.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
4.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Geloy XTPM309E ASA+PC (Europe-Africa-Middle East) XTPM309E is a high heat resistant ASA+PC. It shows high impact retention, which can be positioned for various outdoor and indoor applications requiring superior heat aging properties and colour stab.. |
|||
Melt Flow | 4.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
PolyOne Dynaflex™ G2703-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2703-1000-00 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance and a low coefficient of friction. - Adhesion to Polypropylen.. |
|||
Melt Flow | 4.0 - 6.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.0 - 6.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 4431S (30405) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 4.0 g/10 min @Load 3.80 kg, Temperature 230 °C |
4.0 g/10 min @Load 8.38 lb, Temperature 446 °F |
Cond I; ASTM D1238 |
Ravago Manufacturing Americas Hylac® GP48 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Melt Flow | 4.0 g/10 min @Load 10.0 kg, Temperature 230 °C |
4.0 g/10 min @Load 22.0 lb, Temperature 446 °F |
ASTM D1238 |
Solvay Specialty Polymers Solef® 61010 PVDF Copolymer
(discontinued **) Key features of this grade: Permanent Plasticizing, Fuel Line, Piping, Formulated. Recommended processing is extrusion. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF i.. |
|||
Melt Flow | 4.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
EVALCA EVAL® EP-F104BW Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 32 mol % Ethylene.Data provided by EVALCA. Applications: Cast film, blow molding, tubes, coex coating. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL.. |
|||
Melt Flow | 4.0 - 7.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.0 - 7.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
±15% |
Kazanorgsintez PE2NT21-13 High Density Polyethylene Composite Production Method: Copolymerization of eythylene at low pressure in presence of complex catalysts using gaseous-phase method. Application: Composition is intended for injection molding processin.. |
|||
Melt Flow | 4.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238(G) |
LG Chemical ALPHALAC SG910 HIPS High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include housing of electric appliancesCA.. |
|||
Melt Flow | 4.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 (G) |
LG Chemical HIPS MI750L PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
Melt Flow | 4.0 g/10 min @Load 10.0 kg, Temperature 200 °C |
4.0 g/10 min @Load 22.0 lb, Temperature 392 °F |
ISO 1133 |
Kuraray SEPTON® S2007 Thermoplastic Rubber SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are hydrogenated styrenic block copolymers, which exhi.. |
|||
Melt Flow | 4.0 g/10 min @Load 2.16 kg, Temperature 265 °C |
4.0 g/10 min @Load 4.76 lb, Temperature 509 °F |
ASTM D 1238 |
SABIC Innovative Plastics Xenoy® EXXY0113 PBT (Asia Pacific) Blow Moldable Impact modified XENOYThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 4.0 g/10 min @Load 2.16 kg, Temperature 265 °C |
4.0 g/10 min @Load 4.76 lb, Temperature 509 °F |
ASTM D 1238 |
SABIC Innovative Plastics Xenoy® X6800BM PBT Blow moldable, impact modifed XENOYThis data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 4.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
4.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM Test |
Styrolution Luran® S 776 SE ASA Luran S 776 SE is a general purpose extrusion ASA grade with good toughness and strength, used for sheet and profile extrusions.Information provided by STYROLUTION, which is a joint venture between .. |
|||
Melt Flow | 4.0 g/10 min @Load 2.16 kg, Temperature 250 °C |
4.0 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® WP-1041 PC/ABS, Unreinforced Metal Plating Grade High flow PC/ABS material that can be used for automobile R/G door handleInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 4.0 g/10 min @Load 2.16 kg, Temperature 250 °C |
4.0 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® WP-1041 PC/ABS, Unreinforced Metal Plating Grade High flow PC/ABS material that can be used for automobile R/G door handleInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 4.0 g/10 min @Load 5.00 kg, Temperature 280 °C |
4.0 g/10 min @Load 11.0 lb, Temperature 536 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Noryl LS175 PPE+HIPS (Europe-Africa-Middle East) Noryl* LS175 modified polyphenylene ether resin is an unfilled grade suitable for both extrusion and injection molding conversion routes. It uses non-chlorinated, non-brominated FR additives to del.. |
|||
Melt Flow | 4.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133H |
Total PS CPDS 856 Flame Retardant Polystyrene POLYSTYRENE (PS) COMPOUND (CPDS) 856 is a high impact halogen free polystyrene which offers a good balance of rheological and mechanical properties.Main Characteristics:Bromine and Chlorine free,UL9.. |
|||
Melt Flow | 4.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
4.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D 1238 |
Cossa Polimeri ESTADIENE 1016 HT V0 Flame Retardant ABS Acrylonitrile Butadiene StyreneFlame retardant class V0, with PBDE, high thermal resistance, good physical and mechanical characteristics, excellent processabilityInformation provided by Cossa Polim.. |
|||
Melt Flow | 4.0 g/10 min @Load 10.0 kg, Temperature 190 °C |
4.0 g/10 min @Load 22.0 lb, Temperature 374 °F |
ExxonMobil Method |
ExxonMobil Pax-Plus™ 3201 Blown Film Resin Pax-Plus 3201 is a rubber modified high density polyethylene film resin that exhibits excellent impact strength and stress crack resistance. It is used primarily in film where its good tear resista.. |
|||
Melt Flow | 4.0 g/10 min @Load 5.00 kg, Temperature 230 °C |
4.0 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
ExxonMobil PP4031E2 Polypropylene Impact Copolymer Product Description: An impact copolymer resin for extrusion applications with high melt viscosity and excellent rigidity, shock resistance and dimensional stability. It is designed for corrugated .. |
|||
Melt Flow | 4.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
4.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Diamond Polymers DIAMALOY GLY 7510 High Heat ASA Weatherable Polymer Diamaloy GLY 7510 resin is a high gloss, high heat and high impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. This product is rated f1 by UL and be customed.. |
|||
Melt Flow | 4.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
4.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
cm³/10min; ISO 1133 |
DuPont Performance Polymers Hytrel® HTR237BG BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 45 Shore D Lubricated High Viscosity Polyester Elastomer Developed for Blow Molding Hytrel HTR237BG is designed for blow molding or processing techniques requiring high viscosity. It has nominal dur.. |
|||
Melt Flow | 4.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Hytrel® HTR8068 Polyester Elastomer TPC-ET
(Unverified Data**) 44 Shore D Flame Retardant Polyester Elastomer Developed for Extrusion and Injection Molding Information provided by DuPont Performance Polymers |
|||
Melt Flow | 4.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133H |
Total Lacqrene® 851 High Impact Polystyrene
(discontinued **) LACQRENE® 851 is a flame retardant, high impact polystyrene, halogen free rated UL 94 V0 @ 2.5 mm and UL 94 5VA @ 2mm. LACQRENE® 851 offers rheological and mechanics properties which permits larg.. |