Hexcel® HexPly® ES70 120°C Curing Epoxy Matrix, E-glass Balanced fabric 300 g/m2

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer Hexcel
Trade Name HexPly®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® ES70 120°C Curing Epoxy Matrix, E-glass Balanced fabric 300 g/m2.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by HexCel
Mechanical Properties Metric English Comments
Tensile Strength, Yield 450 MPa
65300 psi
Tensile Modulus 20.0 GPa
2900 ksi
Flexural Yield Strength 550 MPa
79800 psi
Flexural Modulus 22.0 GPa
3190 ksi
Shear Strength 55.0 MPa
7980 psi
0°, Short Beam
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature -18.0 °C
12.0 Month

@Temperature -0.400 °F
Descriptive Properties Value Comments
Fiber Volume (%) 50
Tack Life (days) 30