NOVA Chemicals Sclair® 31E LLDPE Extrusion Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Extrusion Grade
Manufacturer NOVA Chemicals
Trade Name Sclair®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Sclair® 31E LLDPE Extrusion Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Excellent tensile properties, excellent impact toughness, outstanding gloss and clarity, excellent processability.Applications: Coating and sheathing.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 0.922 g/cc
0.0333 lb/in³
ASTM D792
Apparent Bulk Density 0.580 g/cc
0.0210 lb/in³
Melt Flow 11.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
11.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 56
56
ASTM D2240
Tensile Strength, Ultimate 12.4 MPa
1800 psi
ASTM D638
Tensile Strength, Yield 10.3 MPa
1490 psi
ASTM D638
Elongation at Break 725 %
725 %
ASTM D638
Flexural Modulus 0.310 GPa
45.0 ksi
ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 91.0 °C
196 °F
ASTM D1525
Brittleness Temperature <= -70.0 °C
<= -94.0 °F
ASTM D696
Electrical Properties Metric English Comments
Electrical Resistivity 5.00e+17 ohm-cm
5.00e+17 ohm-cm
ASTM D257
Dielectric Constant 2.27
2.27
ASTM 1531
Dissipation Factor 0.00010
0.00010
ASTM 1531
Processing Properties Metric English Comments
Melt Temperature 205 °C
401 °F