Solvay Specialty Polymers Kalix® 9950 Polyamide, High Performance (HPPA), 50% Glass Fiber

Category Polymer , Thermoplastic , Nylon
Manufacturer Solvay Specialty Polymers
Trade Name Kalix®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Kalix® 9950 Polyamide, High Performance (HPPA), 50% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Kalix® 9950 is a 50% glass-fiber reinforced high-performance polyamide. It is hot-water moldable and intended for use in components requiring superior mechanical properties and excellent surface quality.Features: Fast Molding Cycle; Good Dimensional Stability; Good Impact Resistance; Good Surface Finish; High Flow; High Stiffness; High Strength; Hot Water Moldability; Low Warpage; Paintable; PlatableUses: Cell Phones; Electrical Parts; Electrical/Electronic Applications; Thin-walled PartsInjection Molding Notes: Kalix® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Kalix® resins be dried prior to molding.Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.60 g/cc
0.0578 lb/in³
ASTM D792
Filler Content 50 %
50 %
Glass Fiber
Water Absorption 0.37 %

@Time 86400 sec
0.37 %

@Time 24.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.0013 cm/cm
0.0013 in/in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0032 cm/cm
0.0032 in/in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength, Yield 245 MPa
35500 psi
ISO 527-2
Elongation at Break 2.3 %
2.3 %
ISO 527-2
Tensile Modulus 18.5 GPa
2680 ksi
ISO 527-2
Flexural Strength 379 MPa

@Strain 3.50 %
55000 psi

@Strain 3.50 %
ISO 178
Flexural Modulus 15.9 GPa
2310 ksi
ISO 178
Izod Impact, Notched (ISO) 15.0 kJ/m²
7.14 ft-lb/in²
Type 1, Notch A; ISO 180
Izod Impact, Unnotched (ISO) 68.0 kJ/m²
32.4 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 262 °C
504 °F
HDT B; Unannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 254 °C
489 °F
Unannealed; ISO 75-2/A
Flammability, UL94 HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
Electrical Properties Metric English Comments
Dielectric Constant 4.15

@Frequency 2.40e+9 Hz
4.15

@Frequency 2.40e+9 Hz
ASTM D2520
4.15

@Frequency 1.00e+9 Hz
4.15

@Frequency 1.00e+9 Hz
ASTM D2520
Dissipation Factor 0.011

@Frequency 2.40e+9 Hz
0.011

@Frequency 2.40e+9 Hz
Method B; ASTM D2520
0.011

@Frequency 1.00e+9 Hz
0.011

@Frequency 1.00e+9 Hz
Method B; ASTM D2520
Processing Properties Metric English Comments
Rear Barrel Temperature 250 °C
482 °F
Front Barrel Temperature 280 °C
536 °F
Melt Temperature 285 - 305 °C
545 - 581 °F
Mold Temperature 80.0 - 120 °C
176 - 248 °F
Drying Temperature 80.0 °C

@Time 14400 - 43200 sec
176 °F

@Time 4.00 - 12.0 hour
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
North America
Color Black; Colors; Natural; White
Form Pellets
Part Marking Code >PAMXD6/66-GF50<
ISO 11469
Processing Technique Injection Molding; Water-Heated Mold Injection Molding
RoHS Compliance RoHS Compliant
Users viewing this material also viewed the following: