Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.890 GPa @Temperature 60.0 °C |
129 ksi @Temperature 140 °F |
ASTM D790 |
LATI LATAN 3E71 Polyoxymethylene Copolymer (POM) with Elastomer
(Unverified Data**) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
Flexural Modulus | 0.890 GPa | 129 ksi | |
Kraton® G1652 + PP blend (20/80) Unmodified polypropylene has high rigidity and good heat resistance, but poor impact resistance, especially at low temperatures. Blending KRATON D and G polymers with PP significantly improves the .. |
|||
Flexural Modulus | 0.890 GPa | 129 ksi | ASTM D790 |
LG Chemical LUPOL TE-5006K Thermoplastic Elastomer Alloy, Weather Resistant LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem |
|||
Flexural Modulus | 0.890 GPa | 129 ksi | 2 mm/min, 64mm span; ISO 178 |
SABIC Innovative Plastics SABIC PPCOMPOUND 5521 PP SABIC® PPcompound 5521 is a mineral filled, impact modified polypropylene TPO. This material combines good flow with exterior automotive weathering stability. The general purpose black color prod.. |
|||
Flexural Modulus | 0.890 GPa | 129 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 391E Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 0.890 GPa | 129 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 391E Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 0.890 GPa | 129 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 391E Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 0.890 GPa | 129 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 391E Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 0.890 GPa | 129 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 391E Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 0.890 GPa | 129 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 391E Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 0.890 GPa | 129 ksi | ISO 178 |
Ascend Performance Materials Vydyne® 49 Nylon 66, Conditioned Vydyne® 49 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp.. |
|||
Flexural Modulus | 0.890 GPa | 129 ksi | ISO 178 |
Ascend Performance Materials Vydyne® 49H NT Nylon 66, Impact Modified, Conditioned Vydyne® 49H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat-stabilized for improved resista.. |
|||
Flexural Modulus | 0.890 GPa | 129 ksi | ISO 178 |
Breplast Bretene SPF Thermoplastic Composite, 40% PP + 60% PE Recovered polypropylene and polyethylene compositeInformation provided by Breplast S.p.A. |