Beijing Evergrow Resources PTFE Extrusion Tube

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Extruded
Manufacturer Beijing Evergrow Resources
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Beijing Evergrow Resources PTFE Extrusion Tube.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features:PTFE extruded tubing is manufactured by high pressure PTFE dispense resin mixed with additive, it is extruded and sintered. According to different demands, the tubing could be opaque or translucent. PTFE is well known for its chemical resistance, not aging, non stick, self-lubrication, insulation and wide working temperature range from -180°C to +260°C. Because of these excellent properties, PTFE has a wide application in fields of chemical, mechanical, electronics, medical and aviation, etc.Applications:Used as wire and cable jacket, inner lined pipes for corrosive fluids and used in hydrochloric acid heat exchanger, etc.Information provided by Beijing Evergrow Resources.
Physical Properties Metric English Comments
Density 2.10 - 2.20 g/cc
0.0759 - 0.0795 lb/in³
apparent
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 20.0 MPa
>= 2900 psi
Elongation at Break >= 200 %
>= 200 %
Electrical Properties Metric English Comments
Dielectric Strength >= 10.0 kV/mm
>= 254 kV/in
Descriptive Properties Value Comments
Residual Lubricant Content (%) <= 0.5