Asahi Kasei Thermylene® P6-16FG-0801 16% Fiber Glass Reinforced, UV Stabilized

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Glass Fiber Filler
Manufacturer Asahi Kasei
Trade Name Thermylene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asahi Kasei Thermylene® P6-16FG-0801 16% Fiber Glass Reinforced, UV Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Asahi Thermofil
Physical Properties Metric English Comments
Specific Gravity 1.02 g/cc
1.02 g/cc
ASTM D792
Melt Flow 3.0 g/10 min
3.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 60.0 MPa
8700 psi
ASTM D638
Flexural Strength 89.6 MPa
13000 psi
ASTM D790
Flexural Modulus 3.45 GPa
500 ksi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 68.9 °C
156 °F
ASTM D648