Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.10 g/cc | 0.0759 lb/in³ | |
Rogers Corporation RO3003 Ceramic-Filled PTFE Composite, High Frequency Circuit Material Features and Benefits: |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | ASTM D792 |
Rogers Corporation RT/duroid® 6202PR High Frequency Laminate Features:Low loss for excellent high frequency performanceTight dielectric constant and thickness controlExcellent electrical and mechanical propertiesExtremely low thermal coefficient of dielectric.. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | true density |
NanoAmor 95%, OD/ID/L: 20-30/5-10 nm/0.5-2 um Short Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | true density |
NanoAmor 95%, OD/ID/L: 20-40/5-10 nm/1-2 um Short Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | true density |
NanoAmor 95%, OD/ID: < 8/2-5 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | true density |
NanoAmor 95%, OD/ID: ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | true density |
NanoAmor 95%, OD/ID: 10-20/5-10 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | true density |
NanoAmor 95%, OD/ID: 20-40/5-10 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | true density |
NanoAmor 95%, OD/ID: 8-15/3-5 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Density | 2.10 - 2.30 g/cc | 0.0759 - 0.0831 lb/in³ | |
Pyrotek Bonded Particle Filtration Media Bonded particle filtration media is a proven and efficient means for removing oxides from molten aluminum and its alloys. This filtration media is available in either high strength alumina oxide or.. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | true density |
NanoAmor 95%, OD/ID: 30-50/5-15 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Density | 2.10 - 2.17 g/cc | 0.0759 - 0.0784 lb/in³ | Average value: 2.14 g/cc Grade Count:22 |
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyperfluoroalkoxyethylene, Molded/Extruded". Each property range of values reported is minimum and max.. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | Apparent |
Gouda Vuurvast B Dense Refractory Brick Description: A dry-pressed fireclay brick for use up to 1300°C.Remarks: This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda.. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | DIN 53479 |
Polyram Metal Cap PPC372B73 Polypropylene, 73% Mineral Filled 73% mineral filled, heavy density polypropylene for molding metallized parts and galvanized coversInformation provided by Polyram Ram On Ind. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | DIN 53479 |
Polyram Metal Cap PPC373B72 Polypropylene, 72% mineral Filled 72% mineral filled, heavy density polypropylene for molding metallized parts and galvanized coversInformation provided by Polyram Ram On Ind. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | |
Zircar Refractory Composites RS-99R Refractory Sheet Type RS-99R boards are prefired and are unaffected by moisture. They stay rigid even if saturated with water.Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI) |
|||
Density | 2.10 - 2.50 g/cc | 0.0759 - 0.0903 lb/in³ | |
Du-Co Ceramics DC-187 Magnesium Oxide Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | |
Arlon AD300A Glass, PTFE and Micro-Dispersed Ceramic Lower Loss and Improved Performance over Traditional AD Series.Information provided by Arlon Materials for Electronics (MED). |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | ASTM D1505 |
Arlon CuClad 6700 Bonding Film Thermoplastic Bonding FilmsSimilar Dk and Df range to many PTFE laminatesBenefits:Can be reheated to remelt and reflow bonding filmExcellent Electrical PropertiesTypical Applications:Stripline Circu.. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | |
BASF Heligoen® Green K 8683 Color Additive Chemical Structure: Cu-phthalocyanine chlorinate Application: Colourant for plastics; PVC-p, PVC-u, PUR, LD-PE, HD-PE, PP, PS, SB, SAN, PMMA, CA/CAB, and UPRecommendations for food applications: BgV.. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | ASTM D792 Method A |
Arlon AD350A PTFE/Woven Fiberglass/Ceramic Filled Composite Tighter Dielectric Tolerance Low Z-Axis Thermal ExpansionCeramic Filled PTFEHigh Thermal ConductivityLarge Panel SizeBenefits:Higher Consistency of PerformanceSuperior PTH AdhesionHeat Dissipation a.. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | |
Arlon AD430 Glass, PTFE and Micro-Dispersed Ceramic High Dielectric Constant for Circuit Militarization & Patch Antenna ApplicationsInformation provided by Arlon Materials for Electronics (MED). |
|||
Density | 2.10 - 2.15 g/cc | 0.0759 - 0.0777 lb/in³ | molded; ASTM D792 |
Guarniflon PTFE G412 Polytetrafluoroethylene 15% Graphite PTFE G Standard Compound with graphite.Properties: Extremely low coefficient of friction. Fairly good compressive strength. Enhanced chemical resistance. Good wear resistance. Good thermal diss.. |
|||
Density | 2.10 - 2.20 g/cc | 0.0759 - 0.0795 lb/in³ | apparent |
Beijing Evergrow Resources PTFE Extrusion Tube Features:PTFE extruded tubing is manufactured by high pressure PTFE dispense resin mixed with additive, it is extruded and sintered. According to different demands, the tubing could be opaque or tra.. |
|||
Density | 2.10 g/cc | 0.0759 lb/in³ | ASTM D792 |
Sumitomo Bakelite North America SI 9002J-1 Silicone Compound SI 9002J-1 is a short fiberglass reinforced silicone molding compound, which offers moderate strength properties, and dimensional stability and excellent long-term thermal stability at elevated temp.. |