Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Flint Hills P5M4R-034 Polypropylene Random Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Flint Hills Resources
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Flint Hills P5M4R-034 Polypropylene Random Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Radiation resistant. Product does not contain animal derived components. Phthalate-free.Applications: Injection Molding: medical devicesInformation Provided by Flint Hills Resources
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 12 g/10 min
12 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 83
83
ASTM D785
Tensile Strength, Yield 26.0 MPa
3770 psi
ASTM D638
Elongation at Yield 13 %
13 %
ASTM D638
Flexural Modulus, 1% Secant 740 MPa
107000 psi
ASTM D790
Izod Impact, Notched 0.400 J/cm

@Temperature 23.0 °C
0.749 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Gardner Impact 26.0 J

@Temperature 23.0 °C
19.2 ft-lb

@Temperature 73.4 °F
ASTM D5420
Tangent Modulus 790 MPa
115000 psi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C
167 °F
ASTM D648