BCC Products BC 9060 Silicone RTV Rubber

Category Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Adhesive/Sealant Grade
Manufacturer BCC Products
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BCC Products BC 9060 Silicone RTV Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BC 9060 is a blue colored, two-component, flowable compound that, regardless of thickness or confinement, cures at room temperature or by application heat. The cured rubber is high strength and high tear with good elongation. Application: BC 9060 is a mold-making material recommended for repetitive production of intricate shapes cast in epoxy or urethane resins. It is also used in the potting of electronic components and in protecting sensitive assemblies against thermal shock and vibration. Deaeration: Air entrapped during the mixing cycle must be removed to eliminate voids in the cured compound. Place the mixture in a vacuum of 29 inches of mercury. The mixture will expand to 4-5 times its original volume, crest and recede approximately to its original level. Continue the deaeration for an additional 1-2 minutes and the material will be ready to use. Cured Compatibility: cure inhibition (poisoning) of BC 9060 may be caused by various materials used in the master pattern. When the BC 9060 comes in contact with such materials as sulphur containing clays, phosphorous, nitrogen containing materials, organometallic salt (Dibutyl-tin dilaurate, etc.) certain organic adhesives and tapes, cure is hindered. This condition is characterized by a gummy appearance in the surface of the silicone rubber at the interface of the silicone and substrate. A pretest of compatibility is recommended for each suspect substrate to determine whether a barrier coat or other inhibition prevention measure is necessary.Information provided by BCC Products, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.26 g/cc
1.26 g/cc
Brookfield Viscosity 10000 cP
10000 cP
Mixed
140000 cP

@Temperature 25.0 °C
140000 cP

@Temperature 77.0 °F
Compound
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
Tensile Strength, Ultimate 5.52 MPa
800 psi
Elongation at Break 200 %
200 %
Tear Strength 15.8 kN/m
90.0 pli
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -59.4 °C
-75.0 °F
Processing Properties Metric English Comments
Cure Time 15.0 min

@Temperature 60.0 °C
0.250 hour

@Temperature 140 °F
10% cure
24.0 min

@Temperature 60.0 °C
0.400 hour

@Temperature 140 °F
90% cure
Pot Life 120 min

@Temperature 25.0 °C
120 min

@Temperature 77.0 °F
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Mix Ratio 10:1 by weight