Kraton® NEXAR™ MD9200 Polymer Barrier Membrane

Category Polymer
Manufacturer Kraton
Trade Name NEXAR™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kraton® NEXAR™ MD9200 Polymer Barrier Membrane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
NEXAR™ sulfonated block copolymer membranes are designed for water transport, filtration and separation. They have a high moisture vapor transportation rate, allowing usage in humidification and dehumidification applications such as water management and breathable fabrics. They have a high resistance to chlorine, making water treatment a target market.This data sheet is for membranes, but MD9200 is also available in solution for coating or laminating purposes.Information provided by Kraton®.
Mechanical Properties Metric English Comments
Tensile Strength at Break 3.40 MPa
493 psi
Wet
7.00 MPa
1020 psi
Dry
Tensile Strength, Yield 9.00 MPa
1310 psi
Dry
Elongation at Break 57 %
57 %
Dry
90 %
90 %
Wet
Elongation at Yield 4.5 %
4.5 %
Dry
Modulus of Elasticity 0.0300 GPa
4.35 ksi
Wet
0.340 GPa
49.3 ksi
Dry
Descriptive Properties Value Comments
Ion Exchange Capacity 2.0 meq/g