Mechanical Properties Metric English Comments
Tear Strength 15.8 kN/m
90.0 pli
Typical
NuSil MED-4980 Liquid Silicone Rubber - Restricted Medical Use
Description: Liquid silicone rubbers, or LSRs, are elastomer systems reinforced with silica. They contain functional polymers of lower average molecular weight and viscosity when compared to high co..
Tear Strength 15.8 kN/m
90.0 pli
Split; ASTM D624
Northstar Polymers MPP-A90A High Performance Polyether
This high performance polyether system is one of a family of polymer systems developed by Northstar Polymers for specific demanding work environments. Urethane elastomers molded with this system ex..
Tear Strength 15.8 kN/m
90.0 pli
Certified
NuSil MED-4815 Liquid Silicone Rubber - Unrestricted Medical Use
Description: Liquid silicone rubbers, or LSRs, are elastomer systems reinforced with silica. They contain functional polymers of lower average molecular weight and viscosity when compared to high co..
Tear Strength 15.8 kN/m
90.0 pli
Certified
NuSil MED-4820 Liquid Silicone Rubber - Unrestricted Medical Use
Description: Liquid silicone rubbers, or LSRs, are elastomer systems reinforced with silica. They contain functional polymers of lower average molecular weight and viscosity when compared to high co..
Tear Strength 15.8 kN/m
90.0 pli
Die B; silicone property; ASTM D624
Arlon A3020-T002-12 Silicone Rubber/Fiberglass Laminate  (discontinued **)
Side 1: cured fusible silicone rubber; Substrate: 25% sinusoidal fiberglass; Side 2: cured fusible silicone rubber; Interleave: 1 mil PE film
Tear Strength 15.8 kN/m
90.0 pli
Die B, Silicone Property; ASTM D624
Arlon A1030-X008-12 0.030" (0.762 mm) Fully Cured Fusible Silicone Rubber - Extruded Fusible Tape  (disco
1 inch width and 36 inches long. Design/Construction: Interleave: Polyester Film Extruded Fusible Tape (Rectangular Cross Section): Fully Cured Fusible Silicone RubberThis data represents typical v..
Tear Strength 15.8 kN/m
90.0 pli
Die B, Silicone Property; ASTM D624
Arlon A3015-R004-12 0.015" (0.381 mm) Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate  
1 inch width and 36 inches long. Design/Construction: Side 1: Cured Fusible Silicone Rubber Substrate: 25% Sinusoidal FiberglassSide 2: Cured Fusible Silicone Rubber Interleave: Polyester Film This..
Tear Strength 15.8 kN/m
90.0 pli
Die C; ASTM D624
Mearthane Durethaneâ„¢ S DS-230A Solid Polyurethane Elastomer
TDI backbone: ester.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, ..
Tear Strength 15.8 kN/m
90.0 pli
Initial Tear Strength
Saint-Gobain CHR® SG15-03(R) High Performance Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape
Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab..
Tear Strength 15.8 kN/m
90.0 pli
Initial Tear Strength
Saint-Gobain CHR® SG23-03(R) Primary Glass-PTFE Backing Acrylic Adhesive Pressure Sensitive Tape
Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab..
Tear Strength 15.8 kN/m
90.0 pli
Die C; ASTM D 624
RTP Company RTP 2800 B-45A Z Thermoplastic Polyolefin Elastomer (TEO) FDA Compliant Ingredients
Tear Strength 15.8 kN/m
90.0 pli
Dow Corning SILASTIC® J RTV SILICONE RUBBER BASE & CURING AGENT
High durometer silicone mold making rubber recommended for use with rigid and foam polyurethane and can be used with polyesters and epoxies.Information provided by Dow Corning
Tear Strength 15.8 kN/m
90.0 pli
[ppiw], Die B, Silicone Property; ASTM D624
Arlon 48106R008 0.008" (0.203 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 1080 FiberglassSide 2: Uncured Silicone RubberInterleave: Polyethylene This data represents typical values for the production mater..
Tear Strength 15.8 kN/m
90.0 pli
silicone property; ASTM D624
Arlon 51106RB015D Silicone Rubber/Fiberglass Laminate
Interleave 2: 3 mil PE; Side 2: cured silicone rubber; Substrate: 7628 fiberglass; Side 1: uncured silicone rubber, Interleave 1: 3 mil PE
Tear Strength 15.8 kN/m
90.0 pli
Arlon CP-498W Bulk Compound
This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Di..
Tear Strength 15.8 kN/m
90.0 pli
Die B; Silicone Property; ASTM D624
Arlon 55102R024 0.024" Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production material and should not be used as material specifications.In..
Tear Strength 15.8 kN/m
90.0 pli
Die B; silicone property; ASTM D624
Arlon 55106R028 Silicone Rubber/Fiberglass Laminate
Interleave: 3 mil PE; Side 2: uncured silicone rubber; Substrate: 162 fiberglass; Side 1: cured silicone rubber
Tear Strength 15.8 kN/m
90.0 pli
[ppiw], Die B, Silicone Property; ASTM D624
Arlon 55106R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 162 FiberglassSide 2: Cured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red silic..
Tear Strength 15.8 kN/m
90.0 pli
[ppiw], Die B, Silicone Property; ASTM D624
Arlon 55108R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 2, Layer 2: Uncured Silicone RubberSide 2, Layer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured Silicone Rubber This data rep..
Tear Strength 15.8 kN/m
90.0 pli
Die B; silicone property; ASTM D624
Arlon 55143R060 Silicone Rubber/Fiberglass Laminate
Interleave: 3 mil PE; Side 2: cured silicone rubber; Substrate: 162 fiberglass; Side 1: cured silicone rubber
Tear Strength 15.8 kN/m
90.0 pli
Die B; silicone property; ASTM D624
Arlon 55146R028 Silicone Rubber/Fiberglass Laminate
Interleave: 3 mil PE; Side 2: uncured silicone rubber; Substrate: 162 fiberglass; Side 1: cured silicone rubber
Tear Strength 15.8 kN/m
90.0 pli
Layer 1, Die B, [ppiw], Silicone Property; ASTM D624
Arlon 55149R028 0.0295" (0.749 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red si..
Tear Strength 15.8 kN/m
90.0 pli
[ppiw], Silicone Property; ASTM D624
Arlon 55276B028 0.0295" (0.749 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone Rubber Substrate: Style 162 FiberglassSide 1: Cured Silicone Rubber This data represents typical values for the production mate..
Tear Strength 15.8 kN/m
90.0 pli
[ppiw], Layer 1, Die B, Silicone Property; ASTM D624
Arlon 55279R033 0.033" (0.838 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red s..
Tear Strength 15.8 kN/m
90.0 pli
Die B, Silicone Property; ASTM D624
Arlon 44141R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave 1: Clear PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1165 Fiberglass Side 2: Uncured Silicone RubberInterleave 2: Blue PolyethyleneThis data represent..
Tear Strength 15.8 kN/m
90.0 pli
Die C; ASTM D 624
RTP Company RTP 2800 B-45A Thermoplastic Polyolefin Elastomer (TEO)  (discontinued **)
Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Tear Strength 15.8 kN/m
90.0 pli
Die B; Silicone Property; Arlon SQA-TMS-029
Arlon 32140R060 0.060" Uncured Silicone Rubber on Release PET
Design/Construction:Interleave: 0.0025" PolyethyleneSide 1: Uncured Silicone RubberCarrier: 0.005" Release PETThis data represents typical values for the production material and should not be use..
Tear Strength 15.8 kN/m
90.0 pli
Die B, Silicone Property; ASTM D624
Arlon 44278R018 0.018" Uncured/Cured/Uncured Silicone Rubber Laminate with Fiberglass Substrate
Design/Construction:Interleave 1: LDPESide 1 Layer 2: Uncured Silicone RubberSide 1 Layer 1: Cured Silicone RubberSubstrate: Style 1165 FiberglassSide 2: Uncured Silicone RubberInterleave: LDPEUL..
Tear Strength 15.8 kN/m
90.0 pli
Die B; silicone property; ASTM D624
Arlon 55276R028 Silicone Rubber/Fiberglass Laminate
Interleave: 3 mil PE; Side 2: uncured silicone rubber; Substrate: 162 fiberglass; Side 1: cured silicone rubber
Tear Strength 15.8 kN/m
90.0 pli
[ppiw], Layer 1, Silicone Property; ASTM D624
Arlon 55279R031 0.031" (0.787 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red s..