Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tear Strength = 90.0 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 15.8 kN/m
90.0 pli
Die B, Silicone Property; ASTM D624
Arlon A3020-R008-16.5 0.020" (0.508 mm) Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate &nb
2 inches width and 50 inches long. Design/Construction: Side 1: Cured Fusible Silicone Rubber Substrate: 25% sinusoidal FiberglassSide 2: Cured Fusible Silicone Rubber Interleave: Polyester Film Th..
Tear Strength 15.8 kN/m
90.0 pli
Die C; ASTM D624
Mearthane Durethaneâ„¢ S DS-230A Solid Polyurethane Elastomer
TDI backbone: ester.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, ..
Tear Strength 15.8 kN/m
90.0 pli
Warp/Longitudinal direction
Saint-Gobain Chemlam® 4 Value Industrial Laminate
Description: The Chemlam® series is the Chemfab® value line of industrial laminates. Chemlam® composites features uniform thickness, multi-layer cast PTFE films laminated to fiber glass rei..
Tear Strength 15.8 kN/m
90.0 pli
Initial Tear Strength
Saint-Gobain CHR® 2819-3(R) Acrylic Adhesive Zone Tape
Specification Notes: 21CFR177.1550 compliant. All data based on a 0.003 inch test sample.Information provided by Saint Gobain Performance Products.
Tear Strength 15.8 kN/m
90.0 pli
Initial Tear Strength
Saint-Gobain CHR® 2829-3(R) Acrylic Adhesive Zone Tape
Specification Notes: 21CFR177.1550 compliant. All data based on a 0.003 inch test sample. Information provided by Saint Gobain Performance Products.
Tear Strength 15.8 kN/m
90.0 pli
Initial Tear Strength
Saint-Gobain CHR® SG15-03(R) High Performance Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape
Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab..
Tear Strength 15.8 kN/m
90.0 pli
Initial Tear Strength
Saint-Gobain CHR® C665 Copper Foil Backing Acrylic Adhesive Pressure Sensitive Tape
Description: Aluminum and copper foil tapes offer high conformability, conductivity, and reflectivity at elevated temperatures. Aluminum is available with a fiberglass laminate for applications requ..
Tear Strength 15.8 kN/m
90.0 pli
Trouser; ASTM D470
Lubrizol Estane® ZHF 95AT3 Thermoplastic Polyurethane, Flame Retardant
Type: Estane® ZHF 95AT3 TPU is a zero halogen flame retardant polyether based thermoplastic polyurethane compound.Features: Outstanding flame retardant properties, especially suited for tray cables..
Tear Strength 15.8 kN/m
90.0 pli
Die C; ASTM D 624
RTP Company RTP 2800 B-45A Z Thermoplastic Polyolefin Elastomer (TEO) FDA Compliant Ingredients
Tear Strength 15.8 kN/m
90.0 pli
Dow Corning SILASTIC® J RTV SILICONE RUBBER BASE & CURING AGENT
High durometer silicone mold making rubber recommended for use with rigid and foam polyurethane and can be used with polyesters and epoxies.Information provided by Dow Corning
Tear Strength 15.8 kN/m
90.0 pli
Die B, Silicone Property; ASTM D624
Arlon 32140R062 0.062" (1.57 mm) Uncured Silicone Rubber on PET Carrier
Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PETAppearance: Red silicone gum on polymer release linerThis data represents typical values for the production ma..
Tear Strength 15.8 kN/m
90.0 pli
[ppiw], Die B, Silicone Property; ASTM D624
Arlon 48106R008 0.008" (0.203 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 1080 FiberglassSide 2: Uncured Silicone RubberInterleave: Polyethylene This data represents typical values for the production mater..
Tear Strength 15.8 kN/m
90.0 pli
Die B; Silicone Property; Arlon SQA-TMS-029
Arlon 51146R050 0.050" Cured/Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 2.5 mil PEThis data represents typical values for the production materi..
Tear Strength 15.8 kN/m
90.0 pli
[ppiw], Silicone Property; ASTM D624
Arlon 55142R040 0.040" (1.02 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass This data represents typical values for the production material. The data should not be use..
Tear Strength 15.8 kN/m
90.0 pli
Die B; silicone property; ASTM D624
Arlon 56276R026 Silicone Rubber/Fiberglass Laminate
Interleave: 3 mil PE; Side 2: uncured silicone rubber; Substrate: 162 fiberglass; Side 1: cured silicone rubber
Tear Strength 15.8 kN/m
90.0 pli
Die B; silicone property; ASTM D624
Arlon 56976R026 Silicone Rubber/Fiberglass Laminate
Interleave: 3 mil PE; Side 1: cured silicone rubber; Substrate: 1564 fiberglass; Side 2: uncured silicone rubber
Tear Strength 15.8 kN/m
90.0 pli
Arlon CP-498W Bulk Compound
This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Di..
Tear Strength 15.8 kN/m
90.0 pli
Die B, Compound Property; ASTM D624
Arlon R37053W007 0.007" (0.178 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1 Interleave: Polyethylene Side 1: Cured Silicone Rubber Substrate: Style 2133 FiberglassSide 2: Cured Silicone RubberSide 2 Interleave: PolyethyleneThis data represents ty..
Tear Strength 15.8 kN/m
90.0 pli
Die B, Silicone Property; ASTM D624
Arlon 32270R060 0.060" (1.52 mm) Uncured Silicone Rubber on PET Carrier
Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PETAppearance: Red silicone gum on polymer release linerThis data represents typical values for the production ma..
Tear Strength 15.8 kN/m
90.0 pli
Die B; Silicone Property; ASTM D624
Arlon 51103R015 0.0150" Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: LDPESide 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone RubberInterleave: LDPEThis data represents typical values for the producti..
Tear Strength 15.8 kN/m
90.0 pli
Die B; Silicone Property; ASTM D624
Arlon 51141R027 0.0270" Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 2.5 mil PESide 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 2.5 mil PEThis data represents typical values ..
Tear Strength 15.8 kN/m
90.0 pli
Die B; silicone property; ASTM D624
Arlon 51276R020 Silicone Rubber/Fiberglass Laminate
Side 1: cured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene
Tear Strength 15.8 kN/m
90.0 pli
Die B, layer 1; ASTM D624
Arlon 55109R028 Silicone Rubber/Fiberglass Laminate
Interleave: 3 mil PE; Layer 2: uncured silicone rubber; Layer 1: cured silicone rubber; Substrate: 162 fiberglass
Tear Strength 15.8 kN/m
90.0 pli
silicone property, side 1; ASTM D624
Arlon 55141R028 Silicone Rubber/Fiberglass Laminate
Interleave: 3 mil PE; Side 1: uncured silicone rubber; Substrate: 162 fiberglass; Side 2: uncured silicone rubber; Interleave 2: 3 mil PE
Tear Strength 15.8 kN/m
90.0 pli
[ppiw], Die B, Silicone Property; ASTM D624
Arlon 55276R026 0.026" (0.660 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone Rubber Substrate: Style 162 FiberglassSide 1: Uncured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red si..
Tear Strength 15.8 kN/m
90.0 pli
cured 72 hrs @ RT
ACC QM 262 QSI Quantum Silicones 60 Durometer Addition Cure Moldmaking Material
QM262 is a two component, room temperature, addition cure silicone material. The cured rubber has excellent mechanical properties, good shelf-life stability, excellent physical properties and resin ..
Tear Strength 15.8 kN/m
90.0 pli
Die C; ASTM D 624
RTP Company RTP 2800 B-45A Thermoplastic Polyolefin Elastomer (TEO)  (discontinued **)
Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Tear Strength 15.8 kN/m
90.0 pli
Die C (graves), 20 in/min; ASTM D624
PolyOne Synprene® RT-3650 Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:Multi-Purpose Thermoplastic ElastomerNaturalApplications:General PurposeInteriorMarket:Consumer GoodsIndustrialProcessing Method:Injection MoldingInformation provided by PolyOne..
Tear Strength 15.8 kN/m
90.0 pli
[ppiw], Silicone Property; ASTM D624
Arlon 55276R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone Rubber Substrate: Style 162 FiberglassSide 1: Cured Silicone RubberProduct Use: Flexible heater insulationAppearance: Red silic..
Tear Strength 15.8 kN/m
90.0 pli
[ppiw], Layer 1, Silicone Property; ASTM D624
Arlon 55279R031 0.031" (0.787 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red s..
Copyright © lookpolymers.com All Rights Reserved