Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 140000 cP @Temperature 25.0 °C |
140000 cP @Temperature 77.0 °F |
Compound |
BCC Products BC 9060 Silicone RTV Rubber BC 9060 is a blue colored, two-component, flowable compound that, regardless of thickness or confinement, cures at room temperature or by application heat. The cured rubber is high strength and high.. |