Loctite® 3526 Acrylic Light Cure Adhesive

Category Polymer , Adhesive , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer Loctite
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Loctite® 3526 Acrylic Light Cure Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Acrylic Light Cure AdhesivesVersatile Loctite® ultraviolet (UV) and visible light curing adhesives can be used in bonding, encapsulating, coating, tacking, and sealing applications. These single component, solvent-free products cure in seconds when exposed to UV/visible light sources. Some light cure adhesives can be combined with activator curing methods to meet specific application requirements.Loctite® 3526 Acrylic Light Cure AdhesiveA visible/UV/heat cure version of 3525. All the properties of 3525 plus low temperature rapid heat cure capabilities (250°F). Fast cure even under low energy sources. Fluorescent. Key Substrates: Glass, metal, thermoset plastic Cure Type: Ultraviolet, visible, heat
Physical Properties Metric English Comments
Brookfield Viscosity 17800 cP

@Temperature 25.0 °C
17800 cP

@Temperature 77.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 62
62
Elongation at Break 185 %
185 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 149 °C
300 °F
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Descriptive Properties Value Comments
Color Clear/Pale Straw/Fluorescent