BASF Ultramid® HFX 33 PA6 (Dry)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer BASF
Trade Name Ultramid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultramid® HFX 33 PA6 (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Ultramid HFX 33 is a polyamide specialty extrusion resin combining high flexibility, excellent burst performance and outstanding chemical resistance. It offers high melt strength and enhanced heat stability.Applications: Ultramid HFX 33 is recommended for tubing applications requiring an outstanding balance of flexibility, chemical and heat resistance and burst performance.Information provided by BASF
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 38.0 MPa
5510 psi
ISO 527
Elongation at Break 160 %
160 %
Nominal; ISO 527
Tensile Modulus 0.494 GPa
71.6 ksi
ISO 527
Flexural Modulus 0.480 GPa
69.6 ksi
ISO 178
Izod Impact, Notched (ISO) 101 kJ/m²
48.1 ft-lb/in²
ISO 180
Charpy Impact, Notched 11.7 J/cm²
55.7 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 40.0 °C
104 °F
ISO 75
Processing Properties Metric English Comments
Zone 1 225 - 245 °C
437 - 473 °F
Rear
Zone 2 225 - 250 °C
437 - 482 °F
Middle
Zone 3 225 - 245 °C
437 - 473 °F
Front
Zone 4 230 - 245 °C
446 - 473 °F
Head
Zone 5 230 - 245 °C
446 - 473 °F
Flange
Die Temperature 230 - 245 °C
446 - 473 °F
Melt Temperature 225 - 245 °C
437 - 473 °F
Dry Time 2 - 4 hour
2 - 4 hour
Moisture Content <= 0.10 %
<= 0.10 %
Descriptive Properties Value Comments
Commercial Status North America