Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 2 | 225 °C | 437 °F | Metering Zone |
Lubrizol Advanced Materials PEARLTHANE® 11H94 Thermoplastic Polyurethane Elastomer PEARLTHANE® D11H94 is a high performance polycaprolactone copolyester based TPU, supplied in form of translucent, colorless pellets, featuring adequate hardness as well as excellent flow and mech.. |
|||
Zone 2 | 225 - 265 °C | 437 - 509 °F | |
Lehmann & Voss LUVOCOM® NY-4/PL/15/BK Polyamide 612, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3020GX6 Glass Fiber Reinforced Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: conductive, glass fiber reinforced, UV resistanceInformation provided by UBE. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3020GX9 23% Glass Fiber Reinforced Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: 23% glass fiber reinforced gradeInformation provided by UBE. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3020LU1X3 Rigid Black Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3020X15 Nylon 12 Thermister Description: UBESTA Nylon 12 ThermisterInformation provided by UBE. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3020X25L Rigid Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: for coating steel and aluminumInformation provided by UBE. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030JI7 Plasticized Industrial Grade Nylon 12 Description: UBE UBESTA® Industrial grade Nylon 12Comments: low migrationInformation provided by UBE. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030JLX1 Plasticized Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: UV resistance, heat resistanceInformation provided by UBE. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Ethanol for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Ethylacetate for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Ethylene Glycol for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Ethylene Glycol for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Fuel C for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Methyl Ethyl Ketone for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Saturate Sodium Chloride for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030JLX2 Plasticized Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: semi-plasticized, UV resistance, heat resistanceInformation provided by UBE. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030JNU Short Cycle Time Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030LUX Rigid Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: UV resistance, heat resistanceInformation provided by UBE. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Acetic Acid (10%) for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Toluene for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Toluene for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Zinc chloride aq. for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 225 - 300 °C | 437 - 572 °F | |
Akro-Plastic Akromid® B3 GF 50 RM-M (3146) PA 6 Dry, 50% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Zone 2 | 225 - 300 °C | 437 - 572 °F | |
Akro-Plastic Akromid® B3 GF 60 (2476) PA 6 Dry, 60% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Zone 2 | 225 - 250 °C | 437 - 482 °F | Middle |
BASF Ultramid® HFX 33 PA6 (Dry) Description: Ultramid HFX 33 is a polyamide specialty extrusion resin combining high flexibility, excellent burst performance and outstanding chemical resistance. It offers high melt strength and en.. |
|||
Zone 2 | 225 - 300 °C | 437 - 572 °F | |
Akro-Plastic Akromid® B3 GF 30 9 RM-M (3099) PA 6 Dry, 30% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Zone 2 | 225 - 300 °C | 437 - 572 °F | |
Akro-Plastic Akromid® B3 GF 50 9 RM-M (3147) PA 6 Dry, 50% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Zone 2 | 225 - 235 °C | 437 - 455 °F | Extrusion Molding |
LG Chemical KEYFLEX BT S5035 Ester Type TPE Description: Injection Molding, TPC-ET, Airbag Cover Deployment, Medium Modulus, Black ColorApplication: Airbag Cover (DAB, PAB, KAB, SAB)CAS: 37282-12-5, 24968-12-5 and 1333-86-4Information provide.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Xylene for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |