Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 5 | 230 - 245 °C | 446 - 473 °F | Flange |
BASF Ultramid® HFX 33 PA6 (Dry) Description: Ultramid HFX 33 is a polyamide specialty extrusion resin combining high flexibility, excellent burst performance and outstanding chemical resistance. It offers high melt strength and en.. |
|||
Zone 5 | 230 - 245 °C | 446 - 473 °F | Flange |
BASF Ultramid® HFX 35 PA6 (Dry) Description: Ultramid HFX 35 is a polyamide specialty extrusion resin combining high flexibility, outstanding chemical resistance and enhanced heat stability.Applications: Ultramid HFX 35 is recomme.. |
|||
Zone 5 | 230 - 245 °C | 446 - 473 °F | Flange |
BASF Ultramid® HFX 37 PA6 (Dry) Description: Ultramid HFX 37 is a polyamide specialty extrusion resin combining high flexibility, excellent burst performance and outstanding chemical resistance. It offers high melt strength and en.. |
|||
Zone 5 | 230 - 245 °C | 446 - 473 °F | Head |
BASF Nypel® 2351 HS BK PA6 (Dry) Description: Nypel® 2351 HS BK is a heat stabilized, pigmented black, impact modified PA6 extrusion grade compound. Quality and performance are combines at a lower cost. It is based on recycled PA6.. |