Polymer Property : Charpy Impact, Notched = 11.7 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 11.7 J/cm²
55.7 ft-lb/in²
ISO 179
BASF Ultramid® HFX 33 PA6 (Dry)
Description: Ultramid HFX 33 is a polyamide specialty extrusion resin combining high flexibility, excellent burst performance and outstanding chemical resistance. It offers high melt strength and en..