Material Notes:
Tarflen SM1 reinforced with 60% bronze for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Physical Properties Metric English Comments
Density 3.90 g/cc
0.141 lb/in³
ISO 1183
Filler Content 60 %
60 %
Bronze Filler
Particle Size 40 µm
40 µm
Average
Mechanical Properties Metric English Comments
Hardness, Shore D 64
64
ISO 868
Ball Indentation Hardness 52.0 MPa
7540 psi
ISO 2039-1
Tensile Strength, Yield 15.0 MPa
2180 psi
ISO 527
Elongation at Break 220 %
220 %
ISO 527
Izod Impact, Notched 1.40 J/cm
2.62 ft-lb/in
ISO 180
Thermal Properties Metric English Comments
CTE, linear 65.0 µm/m-°C

@Temperature 20.0 °C
36.1 µin/in-°F

@Temperature 68.0 °F
ASTM E 831
Melting Point 327 °C
621 °F
Flammability, UL94 V-0
V-0
Processing Properties Metric English Comments
Processing Temperature 360 °C
680 °F
Molding
Back Pressure 60.0 - 80.0 MPa
8700 - 11600 psi
Molding Pressure
Copyright © lookpolymers.com All Rights Reserved