Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 3.90 g/cc | 0.141 lb/in³ | |
Nabaltec NABALOX® NO 103 Calcined Aluminum Oxide NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | |
Nabaltec NABALOX® NO 105 Calcined Aluminum Oxide NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | |
Nabaltec NABALOX® NO 105-71 RA Calcined Aluminum Oxide NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | |
Nabaltec NABALOX® NO 115 TC Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | |
Nabaltec NABALOX® NO 115-25 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | |
Nabaltec NABALOX® NO 115-G Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | |
Nabaltec NABALOX® NO 135 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | |
Nabaltec NABALOX® NO 313 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | |
Nabaltec NABALOX® NO 315 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | |
Nabaltec NABALOX® NO 325 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | |
Nabaltec NABALOX® NO 625-10 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | |
Nabaltec NABALOX® NO 713-10 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | |
Nabaltec NABALOX® NO 713-40 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | Sintered moldings; ASTM D4894/D4895 |
3M Dyneon™ TF 4406 PTFE, 60% Bronze Filled
(discontinued **) Type II PTFE. Applications include sliding surfaces, bearings.Data provided by Dyneon. |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | ASTM 1457-62 T |
Fluorseals PTFE 60% bronze filled Improved compressive strength and thermal conductivity.Information provided by TEKU GmbH Fluorkunststoffe, a distributor of Fluorseals materials. |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | |
MarkeTech Repton 006 Aluminum Oxide Brand 006 features: Ultra High Purity.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when ther.. |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | |
Misumi Alumina 99 Aluminum Oxide, Al2O3 Information provided by MISUMI Corporation. |
|||
Density | 3.89 g/cc | 0.141 lb/in³ | |
Ferro IP 730 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6 0390 BK Availability: North AmericaForms: PelletsFeatures: High Specific GravityAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | DIN EN 623-2 / ASTM-C373 / ASTM-C20 |
CeramTec Rubalit® 710 Alumina, 99.6% Rubalit® 710 (99.6%) is an alumina that produces optimum results and is considered the material of choice for thin-film technology. Its characterizing features are high strength and thermal conduct.. |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | ASTM C20 |
CoorsTek AD-995 Alumina (nom. 99.5% Al2O3) Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | ASTM-C 20 |
CoorsTek AD-996 99.6% Alumina |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | ASTM-C373 |
CoorsTek ADS-995R MidFilm™ 99.5% Alumina Thick Film Applications: thick films and lasers |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | ASTM-C 20 |
CoorsTek CAP 3 99.5% Alumina Ceramic Armor Material CoorsTek CeraShield™ ceramics provide: low weight, high hardness, controlled, uniform microstructure, dimensional stability over wide temperature range, compatibility for use in finished armor sys.. |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | |
3M Nextel™ 610 Composite Ceramic Fiber Chemical composition above is wt%. Filament diameter is 10-12 µm.3M Nextel Ceramic Fibers 610, 650, and 720 are composite grade fibers. They have a refined crystal structure based on alpha-Al2O3 .. |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | |
BASF Sicotan® Yellow L 1916 Color Additive Description: Transparent yellow iron oxideChemical Structure: Iron Oxide HydrateSuitable for: Waterborn systems, Acrylic-isocyanate systems, Acid curing system, Amine curing system and Airdrying sys.. |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | |
3M Nextel™ DF-11 Woven Fabric 610 Information provided by 3M |
|||
Density | 3.90 g/cc | 0.141 lb/in³ | ISO 1183 |
Azoty Tarnow™ TARFLEN SM-B60 PTFE Tarflen SM1 reinforced with 60% bronze for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Density | >= 3.90 g/cc | >= 0.141 lb/in³ | |
Advanced Ceramics ACL 1091 (C-799) Alumina Information provided by Advanced Ceramics Limited (ACL) |