Processing Properties | Metric | English | Comments |
---|---|---|---|
Back Pressure | 60.0 - 120 MPa | 8700 - 17400 psi | |
Zhejiang Juner 301-G20 20% Glass Fibre Reinforced and Flammable Resistant Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, .. |
|||
Back Pressure | 60.0 - 120 MPa | 8700 - 17400 psi | |
Zhejiang Juner 301-G30 30% Glass Fibre Reinforced and Flammable Resistant Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, .. |
|||
Back Pressure | 60.0 - 80.0 MPa | 8700 - 11600 psi | Molding Pressure |
Azoty Tarnow™ TARFLEN SM-B60 PTFE Tarflen SM1 reinforced with 60% bronze for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |