Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 52.0 MPa | 7540 psi | DIN 53456 |
Global PP-3375-RM Polypropylene Random Copolymer Description-medium stiffness, low melting temperatures, very good for seal Applications-fabricsInformation provided by Global Polymers Corporation. |
|||
Ball Indentation Hardness | 52.0 MPa | 7540 psi | DIN 53456 |
Global PP-3370-RM Polypropylene Random Copolymer Description-medium stiffness, low melting temperatures, very good for seal Applications-filmInformation provided by Global Polymers Corporation. |
|||
Ball Indentation Hardness | 52.0 MPa | 7540 psi | ISO 2039-1 |
Azoty Tarnow™ TARFLEN SM-G15 PTFE Tarflen SM1 reinforced with 15% graphite for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Ball Indentation Hardness | 52.0 - 56.0 MPa | 7540 - 8120 psi | ISO 2032-N961 |
Adamas Adalon® 113 PTFE, 23/2% Carbon/Graphite Filled Information provided by Adamas, HPM |
|||
Ball Indentation Hardness | 52.0 MPa | 7540 psi | 132 N; ISO 2039-1 |
Azoty Tarnow™ TARNOFORM 300 HI6 POM Rubber modified grade with very high impact strength and damping capacity.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Ball Indentation Hardness | 52.0 - 56.0 MPa | 7540 - 8120 psi | ISO 2032-N961 |
Adamas Adalon® 131 PTFE, 25% Soft Carbon Filled Information provided by Adamas, HPM |
|||
Ball Indentation Hardness | 52.0 MPa | 7540 psi | ISO 2039-1 |
Azoty Tarnow™ TARFLEN SM-B60 PTFE Tarflen SM1 reinforced with 60% bronze for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |