Material Notes:
Phenyl silane - C.T.L "37-9X". Graphite fabric - "WCB"
Physical Properties Metric English Comments
Density 1.33 g/cc
0.0480 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 77.22 MPa
11200 psi
Flexural Yield Strength 137 MPa
19900 psi
Flexural Modulus 10.9 GPa
1580 ksi
Compressive Yield Strength 79.3 MPa
11500 psi
Compressive Modulus 13.4 GPa
1940 ksi