Material Notes:
Description: Pluracol® 2090 polyol is a high molecular weight, primary hydroxyl terminated triol. The combination of high molecular weight and reactivity makes Pluracol 2090 useful in the preparation of flexible molded foams. Pluracol 2090 has been formulated with a specialty inhibitor package which is not recommended for flexible slabstock foam production.Information provided by BASF
Physical Properties Metric English Comments
Density 0.993 g/cc

@Temperature 60.0 °C
0.0359 lb/in³

@Temperature 140 °F
1.01 g/cc

@Temperature 37.8 °C
0.0365 lb/in³

@Temperature 100 °F
1.02 g/cc

@Temperature 25.0 °C
0.0368 lb/in³

@Temperature 77.0 °F
Viscosity 280 cP

@Temperature 60.0 °C
280 cP

@Temperature 140 °F
570 cP

@Temperature 37.8 °C
570 cP

@Temperature 100 °F
950 cP

@Temperature 25.0 °C
950 cP

@Temperature 77.0 °F
Molecular Weight 5500 g/mol
5500 g/mol
Thermal Properties Metric English Comments
Specific Heat Capacity 1.16 J/g-°C
0.277 BTU/lb-°F
Thermal Conductivity 0.125 W/m-K
0.868 BTU-in/hr-ft²-°F
Chemical Properties Metric English Comments
Total Acid Number <= 0.010
<= 0.010
STI 3063/3161
Processing Properties Metric English Comments
Moisture Content <= 0.050 %
<= 0.050 %
STI 3062
Descriptive Properties Value Comments
Color <30
APHA, STI 3057
Clear Liquid
Composition Na & K
<5 ppm, STI 3038
Hydroxyl Number 26 - 30 mg KOH/g
STI 3007/3162