Processing Properties Metric English Comments
Processing Temperature 360 °C
680 °F
Average value: 360 °C Grade Count:3
Overview of materials for Polytetrafluoroethylene (PTFE), Bronze Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Bronze Filled". Each property range of values reported is minimum and ma..
Processing Temperature 360 °C
680 °F
Molding
Azoty Tarnow™ TARFLEN SM-B30 PTFE
Reinforced with 30% bronze for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Processing Temperature 360 °C
680 °F
Molding
Azoty Tarnow™ TARFLEN SM-B40 PTFE
Reinforced with 40% bronze for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Processing Temperature 360 °C
680 °F
Molding
Azoty Tarnow™ TARFLEN SM-B60 PTFE
Tarflen SM1 reinforced with 60% bronze for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.