Material Notes:
Georgia Gulf 7045 is a special purpose rigid PVC profile extrusion compound designed for applications requiring the following properties: Impact Strength & ToughnessFlame RetardantColorabilityDimensional StabilityChemical ResistantDurabilityInformation provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
Natural; ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 108
108
ASTM D-785
Hardness, Shore D 79
79
ASTM D-2240
Tensile Strength, Yield 44.8 MPa
6500 psi
ASTM D-638
Tensile Modulus 2.76 GPa
400 ksi
ASTM D-638
Flexural Strength 86.2 MPa
12500 psi
ASTM D-790
Flexural Modulus 2.76 GPa
400 ksi
ASTM D-790
Izod Impact, Notched 10.7 J/cm

@Thickness 3.17 mm
20.0 ft-lb/in

@Thickness 0.125 in
ASTM D-256
Tensile Impact Strength 158 kJ/m²
75.0 ft-lb/in²
ASTM D-1822
Thermal Properties Metric English Comments
CTE, linear 72.0 µm/m-°C

@Temperature 20.0 °C
40.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Deflection Temperature at 1.8 MPa (264 psi) 72.2 °C
162 °F
ASTM D-648
Flammability, UL94 V-0
V-0
At 0.025 inch
Descriptive Properties Value Comments
Cell Classification 14424333
ASTM D-4216