Solvay TECHNYL® A 218W V30 Natural PA66, 30% glass fiber, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Solvay
Trade Name Technyl®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® A 218W V30 Natural PA66, 30% glass fiber, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: TECHNYL® A 218W V30 Nat is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural color.Benefits: The product offers an outstanding long term heat resistance and is suitable to work in environments characterized by a very high temperature. The product offers an improved hydrolisis resistance, as well as an excellent combination between thermal and mechanical properties. It also restricts electrolytical corrosion.Available in: Asia Pacific and EuropeRegulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications.Applications: This grade is recommended for the production of mechanical components in permanent or intermittent contact with hot water, such as electro-magnetic valves. It can also be used as insulation material for electronic connectors, due to its limited electrolytical corrosion.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 135 MPa
19600 psi
ISO 527 Type 1A
Elongation at Break 4.0 %
4.0 %
ISO 527 Type 1A
Tensile Modulus 7.50 GPa
1090 ksi
ISO 527 Type 1A
Flexural Modulus 6.50 GPa
943 ksi
ISO 178
Izod Impact, Notched (ISO) 17.0 kJ/m²
8.09 ft-lb/in²
ISO 180/1eA
Charpy Impact Unnotched 9.50 J/cm²
45.2 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 1.50 J/cm²
7.14 ft-lb/in²
ISO 179/1eA
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Constant 4.3
4.3
IEC 60250
Dielectric Strength 40.0 kV/mm
1020 kV/in
IEC 60243
Dissipation Factor 0.080
0.080
IEC 60250
Comparative Tracking Index 600 V
600 V
Solution A; IEC 60112
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %