Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
SABIC Innovative Plastics Lexan® BFL4000U PC (Asia Pacific) Lexan* BFL4000U Polycarbonate resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating and good impact/flow balance. Designed fo.. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
Ravago Manufacturing Americas Hylon® N2233HL BK Nylon 6 Available in North America Filler: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer and Lubricant Features: Lubricated and Heat StabilizedRoHS CompliantForm: Pellets Proces.. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
PolyOne Geon™ L4605 Green 5765 Polyvinyl Chloride, Semi-Rigid (PVC, Semi-Rigid) Information provided by PolyOne |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
S&E Specialty Polymers TufTech™ GA-8705-03A PVC Compound Application: 80°C Riser Jacketing Compound.Information provided by S&E Specialty Polymers |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Flexible 90057 Polyvinyl Chloride, Flexible (PVC, Flexible) Automotive OEM approval(s).Information provided by PolyOne |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Flexible FC800 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | Method A; ASTM D792 |
LNP Thermocomp® EC-1006 Polyetherimide, Carbon Fiber Reinforcement
(discontinued **) Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st.. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1-8491 Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.High dimensionally stab.. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
LG Chemical LUCEL HI510 POM+Rubber, High Impact Feature: Injection Molding, POM+Rubber, High ImpactApplication: Gears, Automobile ClipCAS No. 66455-31-0Information provided by LG Chemical |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | |
Sylvin Technologies 9940-80 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP RFG16S PA 66 LNP* LUBRICOMP* RFG16S is a compound based on Nylon 66 resin containing 5% Graphite, 30% Glass Fiber. Added features of this material include: Heat Stabilized, Wear Resistant. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
Teknor Apex APEX® 4107 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
Teknor Apex APEX® 84128 Polyvinyl Chloride, Flexible Notes: 80°C Insulation; RoHS Compliant Uses: Wire and Cable Applications Forms: PelletsInformation Provided by Teknor Apex |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ ASC-331 Inorganic Antislip Masterbatch Based in Polyethylene DescriptionPOLYBATCH® ASC-331 is an inorganic antislip masterbatch based in polyethylene. ApplicationThis masterbatch was designed for use in moderate to heavy gauge applications to increase film .. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
Chase Plastics CP Pryme® NN133GL (DAM) Nylon 66, 33% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Brown 1028 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 1028 is a brown color concentrate based in polyethylene. This concentrate was designed to provide opacity and color in polyolefin film and molding applications. POLYBATCH® .. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ISO 1183/1 |
A. Schulman FORMION™ FI 226 40% Glass Fiber Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 226 is an injection molding grade, 40% glass fiber reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness.. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
A. Schulman SCHULAMID® 66 GF30H 30% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Treated Pine 60175U/4 Concentrate Based In LLDPE DescriptionPOLYBATCH® 60175U/4 is a treated pine color concentrate containing an optimized blend of color and UV stabilizer based in LLDPE. This concentrate was designed to provide color and UV s.. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
A. Schulman POLYFLAM™ RPP 1174 Talc Filled, Homopolymer Polypropylene DescriptionPolyflam® RPP 1174 is a high performance talc filled homopolymer polypropylene product with UL V0 flammability and 105°C temperature index at 0.81 mm. RPP 1174 is non-dripping and has .. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
DuPont Performance Polymers VESPEL TP-8311 Polyimide Thermoplastic parts from filled PI (polyimide) for balanced mechanical properties and low wear and friction performance in both dry and lubricated high temperature environmentsInformation provided b.. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | Side 1 Silicone Property; Arlon SQA-TMS-024 |
Arlon 19646B025 Silicone Rubber/Fiberglass Laminate Side 1:cured silicone rubber; Substrate: 1523 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil Polyethylene |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | |
Aremco Corr-Paint™ CP3015-GR High Temperature Protective Coating Inorganic, Mixed Oxides Filled These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. Gray-ceramic inorganic coating to 1400°F. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR Suprex Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
A. Schulman SCHULAMID® 66 GF30H 30% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Specific Gravity | 1.38 g/cc | 1.38 g/cc | |
Sylvin Technologies 9812A-70 Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |