Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C | 162 °F | Unannealed; ASTM D648 |
Multibase Multi-Pro® 2502 CU Black Polypropylene Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C @Thickness 3.18 mm |
162 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Extrusion L0148 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: Finished part testing is required for ASTM E-84 certification. Note: The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by Po.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C @Thickness 3.18 mm |
162 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Dry Blend E6001 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C @Thickness 6.35 mm |
162 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Fittings M1000 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C @Thickness 6.35 mm |
162 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Fittings M1005 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C | 162 °F | ASTM D648 |
Nilit Polynil® P50FIL Super Fast Cycling, Nucleated Nylon 66 Description: Polynil P50 FIL is a nucleated, internally lubricated NYLON 66 with excellent flow characteristics and very fast cycle time. It is widely used throughout many industries for mass produc.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C | 162 °F | Unannealed; ISO 75A-1, -2 |
LyondellBasell Hostacomâ„¢ GP622 Polypropylene Homopolymer Description: Hostacomâ„¢ GP622 high melt flow, 2,900 MPa flexural modulus, 20% talc-filled polypropylene homopolymer is designed for high stiffness and excellent processability in thin-walled par.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C | 162 °F | ASTM D540 |
Spartech PETG 3D Lenticular 3-D Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C | 162 °F | ASTM D648 |
Spartech SP-9070 ABS/PVC Flame Retardant Sheet Description: Flame Retardant SheetInformation provided by Spartech. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C | 162 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Diamond Polymers ABS VP-11 ELG Description: Extrusion Grade, Low Gloss, Flame RetardantInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C | 162 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Diamond Polymers ABS VP-11 SHF Description: High Flow, Flame Retardant ABSInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C | 162 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Diamond Polymers ASA S190 Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C | 162 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Diamond Polymers ASA S910 Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C | 162 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Diamond Polymers ABS VP-11 Description: Flame Retardant ABSInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C | 162 °F | ASTM D648 |
Colorite Polymers 2002 Rigid PVC Description: Colorite Polymers offers a wide range of rigid vinyl compounds for extrusion and injection molding applications for the medical industry. These compounds can be formulated for the produ.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C | 162 °F | ASTM D648 |
Colorite Polymers 2007 Rigid PVC Description: Colorite Polymers offers a wide range of rigid vinyl compounds for extrusion and injection molding applications for the medical industry. These compounds can be formulated for the produ.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C | 162 °F | ASTM D648 |
Colorite Polymers 2007F Rigid PVC Description: Colorite Polymers offers a wide range of rigid vinyl compounds for extrusion and injection molding applications for the medical industry. These compounds can be formulated for the produ.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C | 162 °F | ASTM D648 |
Colorite Polymers 2007NAT Rigid PVC Description: Colorite Polymers offers a wide range of rigid vinyl compounds for extrusion and injection molding applications for the medical industry. These compounds can be formulated for the produ.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C | 162 °F | ASTM D648 |
Colorite Polymers 2018 Rigid PVC Description: Colorite Polymers offers a wide range of rigid vinyl compounds for extrusion and injection molding applications for the medical industry. These compounds can be formulated for the produ.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C | 162 °F | |
Aclo Accutech Polypropylene Homopolymer HP0334W30L1 Wollastonite Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C | 162 °F | ASTM D-648 |
Axiall 7020 Rigid PVC, Extrusion Georgia Gulf 7020 is a special purpose rigid PVC profile extrusion compound designed for thin-wall applications requiring the following properties: Impact Strength & ToughnessDimensional StabilityF.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C | 162 °F | ASTM D-648 |
Axiall 7045 Rigid PVC, Extrusion Georgia Gulf 7045 is a special purpose rigid PVC profile extrusion compound designed for applications requiring the following properties: Impact Strength & ToughnessFlame RetardantColorabilityDimen.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C | 162 °F | ASTM D-648 |
Axiall 7048A Rigid PVC, Extrusion Georgia Gulf 7048A is a general purpose rigid PVC profile extrusion compound designed for applications requiring the following properties: Impact Strength & ToughnessFlame RetardantColorabilityCert.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C | 162 °F | ASTM D-648 |
Axiall 7181 Rigid PVC, Extrusion Georgia Gulf 7181 is a special purpose rigid PVC profile extrusion compound designed for applications requiring the following properties: WeatherabilityImpact StrengthDimensional StabilityFlame Ret.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C | 162 °F | ASTM D-648 |
Axiall 7765 Rigid PVC, Extrusion Georgia Gulf 7765 is a general-purpose indoor rigid PVC profile extrusion compound designed for applications requiring the following properties. 7765 carries an NSF standard 51 listing (for food zo.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C | 162 °F | ASTM D-648 |
Axiall 8247 Clear 34 Rigid PVC, Extrusion, Clear 34 Georgia Gulf 8247 Clear 34 is a rigid PVC pellet compound suited for applications where transparency is important. It is widely used for clear profiles such as furniture trim, shower door and prote.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C | 162 °F | ASTM D-648 |
Axiall 8268 Rigid PVC, Extrusion Georgia Gulf 8268 is a rigid PVC pellet compound suited for applications where transparency is important. It is widely used for clear profiles such as furniture trim, shower door and protected jalo.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C | 162 °F | |
Aclo Accutech Polypropylene Homopolymer HP0339M20L Mica Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C | 162 °F | ASTM D648 |
Colorite Polymers 2019 Rigid PVC Description: Colorite Polymers offers a wide range of rigid vinyl compounds for extrusion and injection molding applications for the medical industry. These compounds can be formulated for the produ.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C | 162 °F | ASTM D-648 |
Axiall 3240 Rigid PVC, Extrusion Georgia Gulf 3240 is a special purpose rigid powder blend PVC compound designed for applications requiring the following properties: WeatherabilityGlossImpact Strength & ToughnessFlame RetardantChe.. |