Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear = 40.0 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 72.0 µm/m-°C

@Temperature -18.0 - 38.0 °C
40.0 µin/in-°F

@Temperature -0.400 - 100 °F
ASTM D696
Plaskolite Duraplex® 50% I Impact Modified Acrylic Sheet
Continuously processed acrylic sheet.Data provided by the manufacturer, Plaskolite, Inc.
CTE, linear 72.0 µm/m-°C

@Temperature -18.0 - 38.0 °C
40.0 µin/in-°F

@Temperature -0.400 - 100 °F
ASTM D696
Plaskolite Duraplex® SG-05 Sign Grade Acrylic Sheet, Impact Modified
Available in unlimited lengths - no seams in finished products.Data provided by the manufacturer, Plaskolite, Inc.
CTE, linear 72.0 µm/m-°C

@Temperature -40.0 - 149 °C
40.0 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Quadrant EPP Nylatron® GS Nylon, Extruded MoS2 Filled Type 66 (ASTM Product Data Sheet)
CTE, linear 72.0 µm/m-°C
40.0 µin/in-°F
ASTM D696
Quantum PBT
Information provided by Quantum Advanced Engineering Plastics
CTE, linear 72.0 µm/m-°C

@Temperature -18.0 - 38.0 °C
40.0 µin/in-°F

@Temperature -0.400 - 100 °F
ASTM D696
Plaskolite Optix® PL-76 Acrylic Resin  (discontinued **)
Injection/extrusion pellets. Medium heat resistance with higher flow than PL-52 pellets.Data provided by the manufacturer, Plaskolite, Inc.
CTE, linear 72.0 µm/m-°C

@Temperature -18.0 - 38.0 °C
40.0 µin/in-°F

@Temperature -0.400 - 100 °F
ASTM D696
Plaskolite Optix® PL-200 Acrylic Resin  (discontinued **)
Injection molding grade pellets.Data provided by the manufacturer, Plaskolite, Inc.
CTE, linear 72.0 - 160 µm/m-°C
40.0 - 88.9 µin/in-°F
Average value: 88.1 µm/m-°C Grade Count:26
Overview of materials for Nylon 46, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
CTE, linear 72.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
40.0 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM-D696
Ineos ABS Lustran® Guardian™ 732 ABS, Extrusion Grade
Lustran® Guardian™ ABS 732 is an extrusion grade resin designed for use in thermoformed refrigerator and freezer liner applications. It is suitable for use with 245fa PU foams.
CTE, linear 72.0 µm/m-°C

@Temperature 20.0 °C
40.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Spartech 513 Static Dissipative Control Sheet
Description: Static Control SheetInformation provided by Spartech.
CTE, linear 72.0 µm/m-°C

@Temperature 20.0 °C
40.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Spartech 617 Static Dissipative Control Sheet
Description: Static Control SheetInformation provided by Spartech.
CTE, linear 72.0 µm/m-°C

@Temperature 20.0 °C
40.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Spartech SP-3010 Rigid PVC Specialty Sheet
Description: Specialty SheetInformation provided by Spartech.
CTE, linear 72.0 µm/m-°C

@Temperature 20.0 °C
40.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Saint-Gobain Norton® ETFE Fluoropolymer Film
Features/Benefits:Superior release propertiesExcellent weatherabilityPerformance from -200°C (-328°F) to 165°C (330°F)Excellent chemical and mechanical propertiesThermoformableProduct th..
CTE, linear 72.0 µm/m-°C
40.0 µin/in-°F
ASTM D 696
Styrolution PS 1600 GPPS
Foam extrusion; Injection moldingGood balanced of strength, flow and heat resistanceFree of zinc and oil additivesInformation provided by Styrolution
CTE, linear 72.0 µm/m-°C
40.0 µin/in-°F
ASTM D 696
Styrolution PS 1621 GPPS
Easy flow material with excellent moldabilityExcellent clarity and set-up timeInformation provided by Styrolution
CTE, linear 72.0 µm/m-°C

@Temperature -40.0 - 82.2 °C
40.0 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
Styron Pulse® 2200BG ABS + PC
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
CTE, linear 72.0 µm/m-°C

@Temperature 0.000 - 100 °C
40.0 µin/in-°F

@Temperature 32.0 - 212 °F
Evonik CYRO Acrylite Plus® H-17 H Acrylic Molding Compound
Data provided by CYRO IndustriesUses: medical devices
CTE, linear 72.0 µm/m-°C

@Temperature 0.000 - 100 °C
40.0 µin/in-°F

@Temperature 32.0 - 212 °F
Evonik CYRO Acrylite Plus® H-17D Acrylic Molding Compound
This material has been replaced by Acrylite Plus® ZK-D - same physical properties with lower haze. Data provided by CYRO IndustriesUses: molded applications
CTE, linear 72.0 µm/m-°C

@Temperature 0.000 - 156 °C
40.0 µin/in-°F

@Temperature 32.0 - 312 °F
ASTM D696
Evonik CYRO ACRYLITE PLUS® ZK-6 Impact Acrylic Polymer
ACRYLITE PLUS® ZK-6 impact acrylic polymer is an amorphous, impact-modified thermoplastic molding and extrusion compound based on polymethyl methacrylate (PMMA).Typical properties of ACRYLITE PLUS®..
CTE, linear 72.0 µm/m-°C

@Temperature 0.000 - 156 °C
40.0 µin/in-°F

@Temperature 32.0 - 312 °F
ASTM D696
Evonik CYRO ACRYLITE PLUS® ZK-F Impact Acrylic Polymer
ACRYLITE PLUS® ZK-F impact acrylic polymer is an amorphous, impact-modified thermoplastic molding and extrusion compound based on polymethyl methacrylate (PMMA).Typical properties of ACRYLITE PLUS®..
CTE, linear 72.0 µm/m-°C

@Temperature 0.000 - 156 °C
40.0 µin/in-°F

@Temperature 32.0 - 312 °F
ASTM D696
Evonik CYRO ACRYLITE PLUS® ZK-X Impact Acrylic Polymer
ACRYLITE PLUS® ZK-X impact acrylic polymer is an amorphous, impact-modified thermoplastic molding and extrusion compound based on polymethyl methacrylate (PMMA).Typical properties of ACRYLITE PLUS®..
CTE, linear 72.0 µm/m-°C

@Temperature 0.000 - 100 °C
40.0 µin/in-°F

@Temperature 32.0 - 212 °F
ASTM D696
Evonik CYRO Acrylite® 8N Acrylic Polymer
CTE, linear 72.0 µm/m-°C

@Temperature 0.000 - 100 °C
40.0 µin/in-°F

@Temperature 32.0 - 212 °F
ASTM D696
Evonik CYRO Acrylite® L40 Compound Molding and Extrusion
Information provided by Cyro Industries
CTE, linear 72.0 µm/m-°C

@Temperature 0.000 - 100 °C
40.0 µin/in-°F

@Temperature 32.0 - 212 °F
ASTM D696
Evonik CYRO XT® Polymer 250 Clear/ Blue Tint Acrylic-Based Multipolymer Compound
XT polymer 250 compound is an impact-modified acrylic-based multipolymer for molding, extrusion and blow molding applications. Typical properties of XT polymer 250 compound are: outstanding thermofo..
CTE, linear 72.0 µm/m-°C

@Temperature 0.000 - 100 °C
40.0 µin/in-°F

@Temperature 32.0 - 212 °F
ISO 11359-2
Evonik CYRO Acrylite® FT15 NTA Compound
CTE, linear 72.0 µm/m-°C

@Temperature 0.000 - 100 °C
40.0 µin/in-°F

@Temperature 32.0 - 212 °F
ASTM D696
Evonik CYRO CYROLITE R30 Acrylic-Based Multipolymer Compound
CTE, linear 72.0 µm/m-°C

@Temperature 20.0 °C
40.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Axiall 7045 Rigid PVC, Extrusion
Georgia Gulf 7045 is a special purpose rigid PVC profile extrusion compound designed for applications requiring the following properties: Impact Strength & ToughnessFlame RetardantColorabilityDimen..
CTE, linear 72.0 µm/m-°C

@Temperature 20.0 °C
40.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Axiall 7801 Rigid PVC, Extrusion, White, High Impact Profile
Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
CTE, linear 72.0 µm/m-°C

@Temperature 20.0 °C
40.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Axiall 3650 Rigid PVC, Extrusion
Georgia Gulf 3650 is a special purpose rigid PVC compound designed for applications requiring the following properties: WeatherabilityGlossImpact Strength & ToughnessFlame RetardantChemical Resistan..
CTE, linear 72.0 - 72.0 µm/m-°C

@Temperature 0.000 - 156 °C
40.0 - 40.0 µin/in-°F

@Temperature 32.0 - 312 °F
Average value: 72.0 µm/m-°C Grade Count:2
Overview of materials for Acrylic, UV Stabilized, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, UV Stabilized, Molded". Each property range of values reported is minimum and maximum values of..
CTE, linear 72.0 µm/m-°C

@Temperature 20.0 °C
40.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Spartech Spectar® UV Copolyester Sheet
Description: Copolyester SheetSpectar is a registered trademark of Eastman Chemical Company.Information provided by Spartech.
Copyright © lookpolymers.com All Rights Reserved